Description: Kraton D1124 P is a clear, branched copolymer based on styrene and isoprene with a polystyrene content of 30%. It is supplied from North America in the physical form identified: Kraton D1124 PT - supplied as a dusted dense pelletRegion: South America, Europe, Asia Pacific, North America, and Japan Uses: Kraton D1124 P is used as an ingredient in formulating adhesives, sealants and coatings. It may also find use as a modifier of bitumen or thermoplastics and in compound formulations.Applications: Adhesives, Sealant and Coatings; Compounding and Personal Hygiene; Impact Modification; Footwear; and Bitumen ModificationInformation provided by Kraton®
Physical Properties Metric English Comments
Specific Gravity 0.940 g/cc
0.940 g/cc
ASTM D4025
Volatiles <= 0.50 %
<= 0.50 %
KM 04
Viscosity 280 - 400 cP
280 - 400 cP
25% Toluene Solution at 25°C; BAM 922
Melt Flow 4.0 g/10 min

@Load 5.00 kg,
Temperature 200 °C
4.0 g/10 min

@Load 11.0 lb,
Temperature 392 °F
Ash 0.15 - 0.35 %
0.15 - 0.35 %
Talc; BAM 908
Mechanical Properties Metric English Comments
Hardness, Shore A 54

@Time 10.0 sec
54

@Time 0.00278 hour
Typical values on polymer compression molded at 300°F; ASTM D2240
Tensile Strength 14.5 MPa
2100 psi
Measured on films cast from a toluene solution; ASTM D412
Elongation at Break 1100 %
1100 %
Measured on films cast from a solution in toluene; ASTM D412
300% Modulus 0.00296 GPa
0.429 ksi
Measured on films cast from a solution in toluene; ASTM D412
Chemical Properties Metric English Comments
Diblock Content 29 %
29 %
Descriptive Properties Value Comments
Content Antioxidant
0.08-0.3%, See Note 1), KM 08
Polystyrene
28.4-31.6%, KM 03
Total Extractables
<1.2%, KM 05
Styrene/Rubber Ratio 30/70