Mechanical Properties Metric English Comments
Tensile Strength 14.5 MPa
2100 psi
ISO 37
Multibase TPSiV® 4200-70A Thermoplastic Elastomer
FEATURES & BENEFITS: Soft silky feel; Excellent abrasion and scratch resistance; Excellent bonding to PC, ABS; Good chemical resistanceAPPLICATIONS: Solution for soft touch overmolding on consumer e..
Tensile Strength 14.5 MPa
2100 psi
ASTM D412
S&E Specialty Polymers TufFlex™ GA-94-244B PVC Compound
Application: 105°C rated vinyl elastomer for medical wire and cable applications. This product complies with the RoHS Directive.Information provided by S&E Specialty Polymers
Tensile Strength >= 14.5 MPa
>= 2100 psi
ASTM D412
S&E Specialty Polymers TufTech™ GA-1038 Natural 85 PVC Compound
Application: A 60 - 75°C general purpose, sunlight resistant compound suitable for jacketing applications.Information provided by S&E Specialty Polymers
Tensile Strength 14.5 MPa
2100 psi
ASTM D412
S&E Specialty Polymers TufTech™ GA-3099LF PVC Compound
Application: RoHS compliant, 80°C AWM insulation and jacketing compoundInformation provided by S&E Specialty Polymers
Tensile Strength 14.5 MPa
2100 psi
ASTM D638
Quadrant EPP Fluorosint® MT-01 Proprietary fluoropolymer reinforced with carbon fibers and organometallic fillers( ASTM Product Data Sheet)
Tensile Strength 14.5 MPa

@Strain 100 %
2100 psi

@Strain 100 %
510 mm/min; ASTM D638
PolyOne Geon™ Vinyl Flexible A4D00 Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne
Tensile Strength 14.5 MPa

@Strain 100 %
2100 psi

@Strain 100 %
510 mm/min; ASTM D638
PolyOne Geon™ Vinyl Flexible A4DU5 Polyvinyl Chloride, Flexible (PVC, Flexible)
Recommended for interior applications.Information provided by PolyOne
Tensile Strength 14.5 MPa

@Strain 100 %
2100 psi

@Strain 100 %
Type IV, 510 mm/min; ASTM D638
PolyOne Geon™ Vinyl Flexible SL9994 Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne
Tensile Strength 14.5 MPa

@Strain 100 %
2100 psi

@Strain 100 %
510 mm/min; ASTM D638
PolyOne Geon™ Vinyl Flexible C5D01 Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne
Tensile Strength 14.5 MPa
2100 psi
ASTM D638
Quadrant EPP Fluorosint® MT-01 Enhanced PTFE (ASTM Product Data Sheet)  (Unverified Data**)
Tensile Strength 14.5 MPa
2100 psi
ISO 37
Kraton® D1124 B (SIS) Branched Triblock Copolymer
Description: Kraton D1124 B is a clear, branched triblock copolymer based on styrene and isoprene with a polystyrene content of 30%. It is supplied from South America in the physical form identified..
Tensile Strength 14.5 MPa
2100 psi
Typical properties on film cast from toluene solution; ASTM D412
Kraton® D1124 K (SIS) Radial Triblock Copolymer
Description: Kraton D1124 K is a clear, radial triblock copolymer based on styrene and isoprene, with a polystyrene content of 30%. It is supplied from North America in the physical form identified:..
Tensile Strength 14.5 MPa
2100 psi
Lucite International Elvacite ® 2046 Acrylic Resin
Elvacite® 2046 is a high molecular weight iso-butyl / n-butyl methacrylate copolymer. Elvacite® 2046 is useful in aluminum finishes, ceramic coatings, and aerosol snows. It is soluble in miner..
Tensile Strength 14.5 MPa
2100 psi
Measured on films cast from a toluene solution; ASTM D412
Kraton® D1124 P (SIS) Branched Copolymer
Description: Kraton D1124 P is a clear, branched copolymer based on styrene and isoprene with a polystyrene content of 30%. It is supplied from North America in the physical form identified: Kraton ..
Tensile Strength 14.5 MPa
2100 psi
ASTM D638
Teknor Apex APEX® 4168 Polyvinyl Chloride Compound
Notes: Sunlight Resistant Jacket Temperature Rating: 75°CInformation Provided by Teknor Apex
Tensile Strength 14.5 MPa
2100 psi
ASTM D638
Ensinger Tecatron® XP-72 Compression Molded PPS Compound, 20% PTFE Filled Natural
Ensinger Special Polymers has over twenty different grades of TECATRON PPS available. Custom formulations can be blended to suit specific applications. Compression molding is amenable to short run p..
Tensile Strength 14.5 MPa
2100 psi
ASTM D638
Ensinger XP-130 Compression Molded PI Compound, 30% PTFE Filled
The XP-130 is an amorphous high performance thermoplastic with high permanent temperature and creep resistance as well as excellent bearing and wear properties, excellent long term thermal stability..
Tensile Strength 14.5 MPa

@Strain 300 %
2100 psi

@Strain 300 %
ISO 37
BASF Elastollan B 80 A TPUR
Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties, outstanding wear resistance, high tensile strength, good damping and resilience performance and sup..
Tensile Strength 14.5 MPa
2100 psi
AlphaGary Megolon™ S340 Low Smoke Halogen Free
Sheathing compound with an LOI of 40+ demonstrating excellent fire performance properties. Application examples include Radio Frequency Cables
Tensile Strength 14.5 MPa
2100 psi
AlphaGary Smokeguard™ HP 700 High Performance Fluoropolymer
Smokeguard™ HP is a high performance fluoropolymer compound with excellent flame and smoke properties intended for difficult constructions and test requirements
Tensile Strength 14.5 MPa
2100 psi
AlphaGary PVC GM 8000-95C Natural LCF Polyvinyl Chloride Thermoplastic
A lead free, 60°C rated, flame retarded, electrical grade molding compound.
Copyright © lookpolymers.com All Rights Reserved