Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 14.5 MPa | 2100 psi | ISO 37 |
Multibase TPSiV® 4200-70A Thermoplastic Elastomer FEATURES & BENEFITS: Soft silky feel; Excellent abrasion and scratch resistance; Excellent bonding to PC, ABS; Good chemical resistanceAPPLICATIONS: Solution for soft touch overmolding on consumer e.. |
|||
Tensile Strength | 14.5 MPa | 2100 psi | ASTM D412 |
S&E Specialty Polymers TufFlex™ GA-94-244B PVC Compound Application: 105°C rated vinyl elastomer for medical wire and cable applications. This product complies with the RoHS Directive.Information provided by S&E Specialty Polymers |
|||
Tensile Strength | >= 14.5 MPa | >= 2100 psi | ASTM D412 |
S&E Specialty Polymers TufTech™ GA-1038 Natural 85 PVC Compound Application: A 60 - 75°C general purpose, sunlight resistant compound suitable for jacketing applications.Information provided by S&E Specialty Polymers |
|||
Tensile Strength | 14.5 MPa | 2100 psi | ASTM D412 |
S&E Specialty Polymers TufTech™ GA-3099LF PVC Compound Application: RoHS compliant, 80°C AWM insulation and jacketing compoundInformation provided by S&E Specialty Polymers |
|||
Tensile Strength | 14.5 MPa | 2100 psi | ASTM D638 |
Quadrant EPP Fluorosint® MT-01 Proprietary fluoropolymer reinforced with carbon fibers and organometallic fillers( ASTM Product Data Sheet) |
|||
Tensile Strength | 14.5 MPa @Strain 100 % |
2100 psi @Strain 100 % |
510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible A4D00 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tensile Strength | 14.5 MPa @Strain 100 % |
2100 psi @Strain 100 % |
510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible A4DU5 Polyvinyl Chloride, Flexible (PVC, Flexible) Recommended for interior applications.Information provided by PolyOne |
|||
Tensile Strength | 14.5 MPa @Strain 100 % |
2100 psi @Strain 100 % |
Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible SL9994 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tensile Strength | 14.5 MPa @Strain 100 % |
2100 psi @Strain 100 % |
510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible C5D01 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tensile Strength | 14.5 MPa | 2100 psi | ASTM D638 |
Quadrant EPP Fluorosint® MT-01 Enhanced PTFE (ASTM Product Data Sheet)
(Unverified Data**) |
|||
Tensile Strength | 14.5 MPa | 2100 psi | ISO 37 |
Kraton® D1124 B (SIS) Branched Triblock Copolymer Description: Kraton D1124 B is a clear, branched triblock copolymer based on styrene and isoprene with a polystyrene content of 30%. It is supplied from South America in the physical form identified.. |
|||
Tensile Strength | 14.5 MPa | 2100 psi | Typical properties on film cast from toluene solution; ASTM D412 |
Kraton® D1124 K (SIS) Radial Triblock Copolymer Description: Kraton D1124 K is a clear, radial triblock copolymer based on styrene and isoprene, with a polystyrene content of 30%. It is supplied from North America in the physical form identified:.. |
|||
Tensile Strength | 14.5 MPa | 2100 psi | |
Lucite International Elvacite ® 2046 Acrylic Resin Elvacite® 2046 is a high molecular weight iso-butyl / n-butyl methacrylate copolymer. Elvacite® 2046 is useful in aluminum finishes, ceramic coatings, and aerosol snows. It is soluble in miner.. |
|||
Tensile Strength | 14.5 MPa | 2100 psi | Measured on films cast from a toluene solution; ASTM D412 |
Kraton® D1124 P (SIS) Branched Copolymer Description: Kraton D1124 P is a clear, branched copolymer based on styrene and isoprene with a polystyrene content of 30%. It is supplied from North America in the physical form identified: Kraton .. |
|||
Tensile Strength | 14.5 MPa | 2100 psi | ASTM D638 |
Teknor Apex APEX® 4168 Polyvinyl Chloride Compound Notes: Sunlight Resistant Jacket Temperature Rating: 75°CInformation Provided by Teknor Apex |
|||
Tensile Strength | 14.5 MPa | 2100 psi | ASTM D638 |
Ensinger Tecatron® XP-72 Compression Molded PPS Compound, 20% PTFE Filled Natural Ensinger Special Polymers has over twenty different grades of TECATRON PPS available. Custom formulations can be blended to suit specific applications. Compression molding is amenable to short run p.. |
|||
Tensile Strength | 14.5 MPa | 2100 psi | ASTM D638 |
Ensinger XP-130 Compression Molded PI Compound, 30% PTFE Filled The XP-130 is an amorphous high performance thermoplastic with high permanent temperature and creep resistance as well as excellent bearing and wear properties, excellent long term thermal stability.. |
|||
Tensile Strength | 14.5 MPa @Strain 300 % |
2100 psi @Strain 300 % |
ISO 37 |
BASF Elastollan B 80 A TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties, outstanding wear resistance, high tensile strength, good damping and resilience performance and sup.. |
|||
Tensile Strength | 14.5 MPa | 2100 psi | |
AlphaGary Megolon™ S340 Low Smoke Halogen Free Sheathing compound with an LOI of 40+ demonstrating excellent fire performance properties. Application examples include Radio Frequency Cables |
|||
Tensile Strength | 14.5 MPa | 2100 psi | |
AlphaGary Smokeguard™ HP 700 High Performance Fluoropolymer Smokeguard™ HP is a high performance fluoropolymer compound with excellent flame and smoke properties intended for difficult constructions and test requirements |
|||
Tensile Strength | 14.5 MPa | 2100 psi | |
AlphaGary PVC GM 8000-95C Natural LCF Polyvinyl Chloride Thermoplastic A lead free, 60°C rated, flame retarded, electrical grade molding compound. |