Mechanical Properties | Metric | English | Comments |
---|---|---|---|
300% Modulus | 0.00296 GPa | 0.429 ksi | ASTM D412 |
Network Polymers Softflex® 0921 Description: Softflex® Thermoplastic Elastomer AlloyInformation provided by Network Polymers Inc. |
|||
300% Modulus | 0.00296 GPa | 0.429 ksi | Typical properties on film cast from toluene solution; ASTM D412 |
Kraton® D1124 K (SIS) Radial Triblock Copolymer Description: Kraton D1124 K is a clear, radial triblock copolymer based on styrene and isoprene, with a polystyrene content of 30%. It is supplied from North America in the physical form identified:.. |
|||
300% Modulus | 0.00296 GPa | 0.429 ksi | Measured on films cast from a solution in toluene; ASTM D412 |
Kraton® D1124 P (SIS) Branched Copolymer Description: Kraton D1124 P is a clear, branched copolymer based on styrene and isoprene with a polystyrene content of 30%. It is supplied from North America in the physical form identified: Kraton .. |
|||
300% Modulus | 0.00296 GPa @Time 7200 sec |
0.429 ksi @Time 2.00 hour |
Die C; ASTM D412 |
STAR Thermoplastic Alloys & Rubbers StarCLEAR CLR-1050 TPE Product Description: StarCLEAR CLR-1050 is an easy processing TPE designed for injection molding. Soft and ultra clear TPEs specifically targeted to medical, consumer and sporting goods market. Feat.. |
|||
300% Modulus | 0.00296 GPa @Time 7200 sec |
0.429 ksi @Time 2.00 hour |
Die C; ASTM D412 |
STAR Thermoplastic Alloys & Rubbers StarXTRUDE XTR-60-1000 TPE Product Description: StarXTRUDE XTR-60-1000 is an easy processing TPE designed for extrusion. Features:Soft TouchRubbery FeelMatte finishExcellent chemical and oil resistanceAdherence to PC, ABS & P.. |