Polymer Property : Tensile Strength, Yield = 13.5 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 13.5 MPa
1960 psi
-10% change after 70 hours @ 100°C; ASTM D412
Precision Polymer Engineering N90B Nitrile Rubber
General purpose, Nitrile Rubber, 85-95 °IRHD. Copolymer of acrylonitrile and butadiene. ASTM & ISO designation = NBR. ASTM D2000 line call-out: M4CH910, A25, B14, EF31, EO15, EO35, F16.Applications..
Tensile Strength, Yield 13.5 MPa
1960 psi
-25% change after 70 hours @ 100°C; ASTM D412
Precision Polymer Engineering Q50Y Polyurethane Rubber
Yellow/Green Polyurethane Rubber, 50-60 °IRHD. ASTM & ISO designation = AU.Applications: Good abrasion resistance and tensile strength, with fluid compatibility approaching that of NBR. Polyuretha..
Tensile Strength, Yield 13.5 MPa
1960 psi
-10% change after 72 hours @ 250°C; ASTM D412
Precision Polymer Engineering V97B Fluoroelastomer Compound
Fluoroelastomer Rubber, 90-98 °IRHD. Terpolymer of vinylidene fluoride, hexafluoropropylene and tetrafluoroethylene. To meet ASTM D2000 line call-out M3HK914, A1-10, B37, B38, EF31, EO78, Z1. Wher..
Tensile Strength, Yield 13.5 MPa
1960 psi
ASTM D412
Teknor Apex ELEXAR® EL 8712 Thermoplastic Elastomer
Information provided by Teknor Apex Company
Tensile Strength, Yield 13.5 MPa
1960 psi
Trelleborg R940 Natural Rubber Polyisoprene
All information provided by Trelleborg
Tensile Strength, Yield 13.5 MPa
1960 psi
after aging 1 week @ 135°C; ASTM D638
Trelleborg Horda Cable E8560 Strippable Semiconductive Shielding
E8560 is a vulcanizing, strippable semiconductive compound, designed for both XLPE and EPDM rubber insulated cables and use in both dry and steam curing processes.E8560 meets the requirements as bel..
Tensile Strength, Yield >= 13.5 MPa
>= 1960 psi
Trelleborg Offshore Vikotherm™ 73780 Insulative Elastomer
Vikotherm™ is a rubber elastomer chemically modified to provide very high insulating characteristics while maintaining its inherent rubber properties in respect of seawater resistance, pressure res..
Tensile Strength, Yield 13.5 MPa

@Strain 300 %
1960 psi

@Strain 300 %
ASTM D412
Dow Buna® SB 1739 Cold polymerized Emulsion Styrene Butadiene Rubber (E-SBR)
Buna® SB 1739 - Schkopau is manufactured by cold polymerization using mixed rosin acid / fatty acid soaps. It is plasticized with 37.5 parts of a TDAE oil in relation to solid rubber. A discolori..
Tensile Strength, Yield 13.5 MPa
1960 psi
ASTM D638
Huntsman PE2065 Injection Molding Polyethylene  (discontinued **)
Homopolymer and FDA compliant.Features: General purpose injection molding resin with good flow characteristicsApplications: Injection molding: lids.FDA Notes: Conforms to FDA regulation 21 CFR 177.1..
Tensile Strength, Yield 13.5 MPa
1960 psi
ASTM D638
Petroquimica Triunfo Trithene® SX 9003 MDPE - Blow Molding
The Trithene® SX 9003 resin is a medium density polyethylene (MDPE) with high molecular weight that presents excellent mechanical properties, thermal stability and high stiffness when compared with..
Tensile Strength, Yield 13.5 MPa
1960 psi
Kraton® D1102 + PP blend (50/50)
Unmodified polypropylene has high rigidity and good heat resistance, but poor impact resistance, especially at low temperatures. Blending KRATON D and G polymers with PP significantly improves the ..