Material Notes:
PTFE powder added, improved wear property. Applications: High speed, high load and wear resistant products. Information provided by API-Kolon.
Physical Properties Metric English Comments
Specific Gravity 1.50 g/cc
1.50 g/cc
ASTM D792
Linear Mold Shrinkage 0.018 cm/cm
0.018 in/in
ASTM D955
Melt Flow 5.0 - 8.0 g/10 min
5.0 - 8.0 g/10 min
ASTM D1238
Ash 18 - 22 %
18 - 22 %
Mechanical Properties Metric English Comments
Hardness, Rockwell M 80
80
ASTM D785
Tensile Strength 41.0 MPa
5950 psi
ASTM D638
Elongation at Break 20 %
20 %
ASTM D638
Flexural Strength 59.0 MPa
8560 psi
ASTM D790
Flexural Modulus 1.764 GPa
255.8 ksi
ASTM D790
Izod Impact, Notched 0.290 J/cm
0.543 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 166 °C
331 °F
ASTM D1525
Flammability, UL94 HB
HB
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+14 ohm-cm
1.00e+14 ohm-cm
ASTM D257
Surface Resistance 1.00e+16 ohm
1.00e+16 ohm
ASTM D257