Kolon ELLAS K-596A Caprolactone Based Thermoplastic Polyurethane

Category Polymer , Thermoplastic , Polyurethane, TP
Manufacturer Kolon
Trade Name ELLAS
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Kolon ELLAS K-596A Caprolactone Based Thermoplastic Polyurethane.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
ApplicationsExtrusionInjectionDust SealOil Seal Information provided by API-Kolon.
Physical Properties Metric English Comments
Specific Gravity 1.18 g/cc
1.18 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 96
96
ASTM D2240
Tensile Strength 52.2 MPa
7570 psi
ASTM D412
Tensile Stress 11.9 MPa

@Strain 100 %
1720 psi

@Strain 100 %
ASTM D412
Elongation at Break 438 %
438 %
ASTM D412
Tear Strength 137 kN/m
784 pli
ASTM D624
Processing Properties Metric English Comments
Nozzle Temperature 190 - 200 °C
374 - 392 °F
Injection Molding
Zone 1 155 - 175 °C
311 - 347 °F
Extrusion Molding
160 - 175 °C
320 - 347 °F
Injection Molding
Zone 2 170 - 180 °C
338 - 356 °F
Extrusion Molding
175 - 185 °C
347 - 365 °F
Injection Molding
Zone 3 180 - 190 °C
356 - 374 °F
Extrusion Molding
185 - 195 °C
365 - 383 °F
Injection Molding
Zone 4 185 - 195 °C
365 - 383 °F
Extrusion Molding
Die Temperature 185 - 195 °C
365 - 383 °F
Extrusion Molding
Head Temperature 190 - 200 °C
374 - 392 °F
Extrusion Molding