Polymer Property : Tensile Strength = 52.2 MPa
Polymer Property :
Tensile Strength =
52.2 MPa
Product List
Mechanical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties
Metric
English
Comments
Tensile Strength
52.2
MPa
7570
psi
ASTM D412
Kolon ELLAS K-596A Caprolactone Based Thermoplastic Polyurethane
ApplicationsExtrusionInjectionDust SealOil Seal Information provided by API-Kolon.