Processing Properties | Metric | English | Comments |
---|---|---|---|
Zone 3 | 180 - 190 °C | 356 - 374 °F | |
Celanese Celcon® LW90 POM, Tribological
(Unverified Data**) Celcon® LW90 is a nominal 9 melt flow rate based material specifically formulated for high speed, low wear applications against metals. LW90 conforms to applicable FDA regulations governing food co.. |
|||
Zone 3 | 180 - 190 °C | 356 - 374 °F | |
Celanese Celcon® M25UV POM, UV Resistant
(Unverified Data**) Celcon® M25UV is an acetal copolymer developed as a natural UV light stabilized low flow, high molecular weight grade. It has been formulated as a natural acetal that does not discolor, yet maintai.. |
|||
Zone 3 | 180 - 190 °C | 356 - 374 °F | |
Celanese Celcon® M50 POM
(Unverified Data**) Celcon® M50 is a extrusion and injection molding grade with an intermediate viscosity for good processability with higher toughness than general purpose grades.Standard extruders with a length to d.. |
|||
Zone 3 | 180 - 190 °C | 356 - 374 °F | |
Celanese Celcon® MC90-HM POM, Mineral Reinforced
(Unverified Data**) Celcon® MC90-HM is a highly mineral filled and coupled M90 material for producing very flat and dimensionally stable parts (normal flow).Mineral coupled for reduced warpage, high modulus, moderate .. |
|||
Zone 3 | 180 - 190 °C | 356 - 374 °F | |
Celanese Celcon® UV270Z POM, UV Resistant
(Unverified Data**) Celcon® UV270Z is a nominal 27 melt flow rate acetal copolymer which has been specially stabilized to prevent discoloration and deterioration of mechanical properties from ultraviolet light exposur.. |
|||
Zone 3 | 170 - 190 °C | 338 - 374 °F | Extrusion Molding |
Kolon ELLAS K-390A Ether Based Thermoplastic Polyurethane ApplicationsExtrusion: Cable Sheathing, high pressure tubeInjectionElectric WireIndustry Parts Information provided by API-Kolon. |
|||
Zone 3 | 175 - 190 °C | 347 - 374 °F | Extrusion Molding |
Kolon ELLAS K-429A Ester Based Thermoplastic Polyurethane ApplicationsIndustry PartsOutsole of Soccer ShoeHighly Pressurized Hose Information provided by API-Kolon. |
|||
Zone 3 | 180 - 190 °C | 356 - 374 °F | Extrusion Molding |
Kolon ELLAS K-480A Ester Based Thermoplastic Polyurethane ApplicationsExtrusionInjectionCompoundingIndustry PartsParts for Automobile/Mobile phoneAcetal Compound Information provided by API-Kolon. |
|||
Zone 3 | 180 - 190 °C | 356 - 374 °F | Extrusion Molding |
Kolon ELLAS K-585A Caprolactone Based Thermoplastic Polyurethane ApplicationsInjectionIndustry Parts Information provided by API-Kolon. |
|||
Zone 3 | 180 - 190 °C | 356 - 374 °F | Extrusion Molding |
Kolon ELLAS K-590A Caprolactone Based Thermoplastic Polyurethane ApplicationsExtrusionInjectionDust SealOil Seal Information provided by API-Kolon. |
|||
Zone 3 | 170 - 190 °C | 338 - 374 °F | Extrusion Molding |
Kolon ELLAS K-787A Ester Based Thermoplastic Polyurethane ApplicationsExtrusionInjectionFlexible HoseIndustry Parts Information provided by API-Kolon. |
|||
Zone 3 | 170 - 190 °C | 338 - 374 °F | |
Silon Taborex TA 1108 HD Chemically-Crosslinkable HDPE Compound TABOREX TA 1108 HD is a crosslinkable compound according to the “SIOPLAS-SYSTEMâ€; made by a Silane grafted ethylene copolymer known as the graft and a Masterbatch containing the crosslinki.. |
|||
Zone 3 | 180 - 190 °C | 356 - 374 °F | |
Celanese Celcon® M90SW POM, Tribological Celcon M90SW is a low wear grade designed for gears and other low wear applications, especially where reducing noise and wear against the same mating surface is important. This grade may be preferre.. |
|||
Zone 3 | 180 - 190 °C | 356 - 374 °F | |
Celanese Celcon® MC90 POM, Mineral Reinforced Celcon« acetal copolymer grade MC90 is a mineral reinforced grade offering low warp, improved dimensional stability, improved stiffness, improved practical impact and retention of other base resin .. |
|||
Zone 3 | 180 - 190 °C | 356 - 374 °F | |
Celanese Celcon® WR90Z POM, UV Resistant Celcon« WR90Z is a standard nominal 9 melt flow rate based acetal copolymer stabilized to provide maximum ultraviolet radiation resistance in outdoor applications while retaining a good balance of .. |
|||
Zone 3 | 180 - 190 °C | 356 - 374 °F | |
Celanese Hostaform® XT 20 POM, Impact Modified Preliminary Data SheetInformation provided by Celanese |
|||
Zone 3 | 180 - 190 °C | 356 - 374 °F | |
Celanese Hostaform® S 9362 XAP2 ™ POM, Impact Modified Preliminary Data SheetDrying is suggested to help achieve low emission performance and to counter if material has contacted moisture through improper storage and handling.Information provided by Cel.. |
|||
Zone 3 | 180 - 190 °C | 356 - 374 °F | |
Celanese Celcon® LW90 POM, Tribological Celcon« LW90 is a nominal 9 melt flow rate based material specifically formulated for high speed, low wear applications against metals. LW90 conforms to applicable FDA regulations governing food co.. |
|||
Zone 3 | 180 - 190 °C | 356 - 374 °F | |
Celanese Celcon® M140-L1 POM, Tribological Celcon« M140-L1 is a general purpose acetal copolymer material with a slightly lower viscosity for improved flow in molding that has been modified to reduce or eliminate noise (squeak) when wearing.. |
|||
Zone 3 | 180 - 190 °C | 356 - 374 °F | |
Celanese Celcon® M25 POM, Unfilled Celcon« acetal copolymer grade M25 is a high molecular weight, higher toughness and impact resistance grade primarily used for extrusion and selected injection molding applications.Information prov.. |
|||
Zone 3 | 180 - 190 °C | 356 - 374 °F | |
Celanese Celcon® M90™ POM, Unfilled Celcon acetal copolymer grade M90Ö is a medium viscosity polymer providing optimum performance in general purpose injection molding and extrusion of thin walled tubing and thin gauge film. This gr.. |
|||
Zone 3 | 180 - 190 °C | 356 - 374 °F | |
Celanese Celcon® MR25B POM, Specialty Celcon« MR25B is a specialty media resistant grade developed for improved bleach resistance and improved toughness.Information provided by Celanese |
|||
Zone 3 | 180 - 190 °C | 356 - 374 °F | |
Celanese Hostaform® S 9363 POM, Impact Modified Hostaform« acetal copolymer grade S 9363 is an impact modified grade for demanding applications. Hostaform« S 9363 provides good impact strength while improving modulus and weld line strength o.. |
|||
Zone 3 | 180 - 190 °C | 356 - 374 °F | |
Celanese Hostaform® S 9363 XAP² ™ POM, Impact Modified Hostaform« acetal copolymer grade S 9363 XAP2 Ö is an impact modified grade for demanding applications. Hostaform« S 9363 XAP2 Ö provides good impact strength while improving modulus and weld.. |
|||
Zone 3 | 180 - 190 °C | 356 - 374 °F | |
Celanese Hostaform® S 9364 XAP² ™ POM, Impact Modified Hostaform« acetal copolymer grade S 9364 XAP2 Ö is highly impact modified grade for demanding applications. Hostaform« S 9364 XAP2 Ö provides a significant improvement in impact strength and fl.. |
|||
Zone 3 | 180 - 190 °C | 356 - 374 °F | |
Celanese Celcon® GC15 POM, 15% Glass Reinforced
(Unverified Data**) Celcon® GC15 is an acetal copolymer grade utilizing a nominal 15 wt. % fiber glass level to increase stiffness and strength.15% glass fibers, coupled for improved stiffnessStandard reciprocating sc.. |
|||
Zone 3 | 180 - 190 °C | 356 - 374 °F | |
Celanese Celcon® GC25TF POM, 25% Glass Reinforced
(Unverified Data**) Celcon® GC25TF is a 25% glass coupled acetal copolymer formulated for higher flow in thin walled and small parts. Celcon GC25TF is also exceptionally resistant to fuel. It offers excellent resista.. |
|||
Zone 3 | 180 - 190 °C | 356 - 374 °F | |
Celanese Celcon® LM90Z POM, Specialty
(Unverified Data**) Celcon® LM90Z is a UV stable, nominal 9 melt flow acetal copolymer which is capable of being permanently marked by a laser. It gives protection against property and color deterioration in applicati.. |
|||
Zone 3 | 180 - 190 °C | 356 - 374 °F | |
Celanese Celcon® M25 POM
(Unverified Data**) Celcon® acetal copolymer grade M25 is a high molecular weight, higher toughness and impact resistance grade primarily used for extrusion and selected injection molding applications.Standard extrude.. |
|||
Zone 3 | 180 - 190 °C | 356 - 374 °F | |
Celanese Hostaform® S 9363 POM, Impact Modified
(Unverified Data**) Hostaform® acetal copolymer grade S 9363 is an impact modified grade for demanding applications. Hostaform® S 9363 provides good impact strength while improving modulus and weld line strength o.. |