Processing Properties | Metric | English | Comments |
---|---|---|---|
Zone 3 | 180 - 190 °C | 356 - 374 °F | |
Celanese Celcon® M140-L1 POM, Tribological
(Unverified Data**) Celcon® M140-L1 is a general purpose acetal copolymer material with a slightly lower viscosity for improved flow in molding that has been modified to reduce or eliminate noise (squeak) when wearing.. |
|||
Zone 3 | 180 - 190 °C | 356 - 374 °F | |
Celanese Celcon® M90UV POM, UV Resistant
(Unverified Data**) Celcon® M90UV is an acetal copolymer developed as a natural UV light stabilized standard flow grade for overall performance in most molding applications. It has been formulated as a natural acetal .. |
|||
Zone 3 | 180 - 190 °C | 356 - 374 °F | |
Celanese Celcon® UV25Z POM, UV Resistant
(Unverified Data**) Celcon® UV25Z is a nominal 2.5 melt flow rate acetal copolymer which has been specially stabilized to prevent discoloration and deterioration of mechanical properties from ultraviolet light exposur.. |
|||
Zone 3 | 180 - 190 °C | 356 - 374 °F | |
Celanese Hostaform® M90LF POM
(Unverified Data**) Hostaform® acetal copolymer grade M90LF is a medium viscosity polymer providing optimum performance in general purpose injection molding and extrusion of thin walled tubing and thin gauge film.Stan.. |
|||
Zone 3 | 170 - 190 °C | 338 - 374 °F | Extrusion Molding |
Kolon ELLAS K-395A Ether Based Thermoplastic Polyurethane ApplicationsExtrusionInjection: Cable sheathing, Highly Pressurized HoseIndustry Parts Information provided by API-Kolon. |
|||
Zone 3 | 180 - 190 °C | 356 - 374 °F | Injection Molding |
Kolon ELLAS K-395A Ether Based Thermoplastic Polyurethane ApplicationsExtrusionInjection: Cable sheathing, Highly Pressurized HoseIndustry Parts Information provided by API-Kolon. |
|||
Zone 3 | 170 - 190 °C | 338 - 374 °F | Extrusion Molding |
Kolon ELLAS K-787A Ester Based Thermoplastic Polyurethane ApplicationsExtrusionInjectionFlexible HoseIndustry Parts Information provided by API-Kolon. |
|||
Zone 3 | 175 - 190 °C | 347 - 374 °F | Extrusion Molding |
Kolon ELLAS K-793AB Ester Based Thermoplastic Polyurethane ApplicationsFilm/SeatBlown filmIndustry Parts Information provided by API-Kolon. |
|||
Zone 3 | 180 - 190 °C | 356 - 374 °F | |
Celanese Celcon® GB10 POM, 10% Glass Reinforced Celcon« GB10 is a 10% glass bead filled grade for low shrinkage and warp resistance in large, flat, and thin walled parts.Information provided by Celanese |
|||
Zone 3 | 180 - 190 °C | 356 - 374 °F | |
Celanese Hostaform® LM90 POM, Specialty Hostaform« LM90 is a nominal 9 melt flow rate acetal copolymer which is capable of being permanently marked by a laser. Parts molded from Hostaform« LM90 can be laser marked with barcodes, identif.. |
|||
Zone 3 | 180 - 190 °C | 356 - 374 °F | |
Celanese Hostaform® S 9362 XAP2 ™ POM, Impact Modified Preliminary Data SheetDrying is suggested to help achieve low emission performance and to counter if material has contacted moisture through improper storage and handling.Information provided by Cel.. |
|||
Zone 3 | 180 - 190 °C | 356 - 374 °F | |
Celanese Celcon® CF802 POM, Specialty Celcon« acetal copolymer grade CF802 is a conductive, fuel compatible general purpose acetal copolymer. Celcon« CF802 has been developed to dissipate static electricity from fuel handling systems... |
|||
Zone 3 | 180 - 190 °C | 356 - 374 °F | |
Celanese Celcon® GC25A POM, 25% Glass Reinforced Celcon« acetal copolymer grade GC25A is a glass coupled formulation containing 25% reinforced fiber glass. This grade offers excellent strength, stiffness and heat distortion temperature with lower.. |
|||
Zone 3 | 180 - 190 °C | 356 - 374 °F | |
Celanese Celcon® M25 POM, Unfilled Celcon« acetal copolymer grade M25 is a high molecular weight, higher toughness and impact resistance grade primarily used for extrusion and selected injection molding applications.Information prov.. |
|||
Zone 3 | 180 - 190 °C | 356 - 374 °F | |
Celanese Celcon® MR25B POM, Specialty Celcon« MR25B is a specialty media resistant grade developed for improved bleach resistance and improved toughness.Information provided by Celanese |
|||
Zone 3 | 180 - 190 °C | 356 - 374 °F | |
Celanese Celcon® UV90Z POM, UV Resistant Celcon« UV90Z is an integrally colored nominal 9 melt flow rate based acetal copolymer material stabilized for use where ultraviolet radiation exposure is to be encountered. The material is formula.. |
|||
Zone 3 | 180 - 190 °C | 356 - 374 °F | |
Celanese Hostaform® S 9363 POM, Impact Modified Hostaform« acetal copolymer grade S 9363 is an impact modified grade for demanding applications. Hostaform« S 9363 provides good impact strength while improving modulus and weld line strength o.. |
|||
Zone 3 | 180 - 190 °C | 356 - 374 °F | |
Celanese Hostaform® S 9364 WS 10/1570 POM, UV Resistant Preliminary Data SheetInformation provided by Celanese |
|||
Zone 3 | 180 - 190 °C | 356 - 374 °F | |
Celanese Hostaform® S 9364 XAP² ™ POM, Impact Modified Hostaform« acetal copolymer grade S 9364 XAP2 Ö is highly impact modified grade for demanding applications. Hostaform« S 9364 XAP2 Ö provides a significant improvement in impact strength and fl.. |
|||
Zone 3 | 180 - 190 °C | 356 - 374 °F | |
Celanese Hostaform® S 9363 XAP2 ™ POM, Impact Modified Preliminary Data SheetDrying is suggested to help achieve low emission performance and to counter if material has contacted moisture through improper storage and handling.Information provided by Cel.. |
|||
Zone 3 | 180 - 190 °C | 356 - 374 °F | |
Celanese Celcon® GB25 POM, 25% Glass Reinforced
(Unverified Data**) Celcon® GB25 acetal copolymer is a 25% glass bead filled grade for low shrinkage and warp resistance in large, flat and thin walled parts.25% glass bead filled for stiffness, low warpageStandard re.. |
|||
Zone 3 | 180 - 190 °C | 356 - 374 °F | |
Celanese Celcon® GC10 POM, 10% Glass Reinforced
(Unverified Data**) Celcon® GC10 acetal copolymer is a 10% glass reinforced acetal for improved strength and stiffness.10% glass fiber, has been replaced with Hostaform® C 9021 GV1/10Standard reciprocating screw inje.. |
|||
Zone 3 | 180 - 190 °C | 356 - 374 °F | |
Celanese Celcon® GC15 POM, 15% Glass Reinforced
(Unverified Data**) Celcon® GC15 is an acetal copolymer grade utilizing a nominal 15 wt. % fiber glass level to increase stiffness and strength.15% glass fibers, coupled for improved stiffnessStandard reciprocating sc.. |
|||
Zone 3 | 180 - 190 °C | 356 - 374 °F | |
Celanese Celcon® GC25TF POM, 25% Glass Reinforced
(Unverified Data**) Celcon® GC25TF is a 25% glass coupled acetal copolymer formulated for higher flow in thin walled and small parts. Celcon GC25TF is also exceptionally resistant to fuel. It offers excellent resista.. |
|||
Zone 3 | 180 - 190 °C | 356 - 374 °F | |
Celanese Celcon® M140 POM
(Unverified Data**) Celcon® acetal copolymer grade M140 is a moderately high flow general purpose injection molding grade. It is designed for use in applications requiring some enhanced flow characteristics over the s.. |
|||
Zone 3 | 180 - 190 °C | 356 - 374 °F | |
Celanese Celcon® WR90Z POM, UV Resistant
(Unverified Data**) Celcon® WR90Z is a standard nominal 9 melt flow rate based acetal copolymer stabilized to provide maximum ultraviolet radiation resistance in outdoor applications while retaining a good balance of .. |
|||
Zone 3 | 180 - 190 °C | 356 - 374 °F | |
Celanese Hostaform® XT 90 POM, Impact Modified
(Unverified Data**) Preliminary Data SheetHighly impact modified, improved weld lineInformation provided by Celanese |
|||
Zone 3 | 180 - 190 °C | 356 - 374 °F | |
Celanese Hostaform® MT12R01 POM, Medical Technology Hostaform« MT12R01 is a special grade developed for medical industry applications containing low residual monomers and no animal products. Hostaform« MT12R01 is a low melt viscosity and improved .. |
|||
Zone 3 | 180 - 190 °C | 356 - 374 °F | |
Celanese Celcon® LW90FS-K POM, Tribological Celcon« acetal copolymer grade LW90FS-K is wear resistant grade of M90 based on both silicone and a high level of PTFE to give excellent slip and wear resistance properties in demanding application.. |
|||
Zone 3 | 180 - 190 °C | 356 - 374 °F | |
Celanese Celcon® MC270 POM, Mineral Reinforced Celcon« MC270 is a mineral coupled acetal copolymer designed for applications requiring improved stiffness, lower mold shrinkage and reduced warpage while maintaining the mechanical performance cha.. |