Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 11.9 MPa @Strain 100 % |
1720 psi @Strain 100 % |
ASTM D412 |
Kolon ELLAS K-596A Caprolactone Based Thermoplastic Polyurethane ApplicationsExtrusionInjectionDust SealOil Seal Information provided by API-Kolon. |