Material Notes:
Production Method: Composition is achieved on the basis of high pressure polyethylene (low density) and low pressure (high density) with stabilizers and other additives. Application: Compositions are used for lapping, cable sheaths, and serving by extrusion method.Information Provided by Kazanorgsintez
Physical Properties Metric English Comments
Volatiles <= 0.070 %
<= 0.070 %
Superior Quality
<= 0.10 %
<= 0.10 %
Premium Quality
Environmental Stress Crack Resistance >= 500 hour
>= 500 hour
Melt Flow 0.21 - 0.39 g/10 min
0.21 - 0.39 g/10 min
±8% Superior Quality, ±12% Premium Quality
Mechanical Properties Metric English Comments
Tensile Strength, Yield >= 9.80 MPa
>= 1420 psi
Elongation at Break >= 600 %
>= 600 %
Tear Strength Test >= 13.7
>= 13.7
MPa
Descriptive Properties Value Comments
Extractable Substance Weight Content (%) 0.5
Superior Quality
0.6
Premium Quality
Copyright © lookpolymers.com All Rights Reserved