Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 9.79 MPa | 1420 psi | ASTM D412 |
Polymax® Maxelast® P3870H TPE, PP Overmold or Standalone use Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti.. |
|||
Tensile Strength, Yield | 9.80 MPa | 1420 psi | ASTM D412 |
Precision Polymer Engineering S55T Silicone Rubber Translucent Silicone Rubber, 45-55 °IRHD. Silicone rubber having both methyl and vinyl substituent groups on the polymer chain. Formulated using only those ingredients determined by the United Sta.. |
|||
Tensile Strength, Yield | 9.80 - 18.2 MPa | 1420 - 2640 psi | ±30% change after 72 hours @ 250°C; ASTM D412 |
Precision Polymer Engineering V80H Fluoroelastomer Compound Fluoroelastomer Rubber, 75-85 °IRHD. Copolymer of vinylidene fluoride and hexafluoropropylene. Formulated using only those ingredients determined by the United States Federal Food and Drug Adminis.. |
|||
Tensile Strength, Yield | >= 9.80 MPa | >= 1420 psi | |
Kazanorgsintez 102-03K Cable Composition Based on Low Density Polyethylene Production Method: Produced in the form of pellets (natural or black colored) on the bases of basic 10204-003, 15303-003, 15313-003. Application: Designed to apply isolation, cable covers and ca.. |
|||
Tensile Strength, Yield | >= 9.80 MPa | >= 1420 psi | |
Kazanorgsintez 102-05K Cable Composition Based on Low Density Polyethylene Production Method: Produced in the form of pellets (natural or black colored) on the bases of basic 10204-003, 15303-003, 15313-003. Application: Designed to apply isolation, cable covers and ca.. |
|||
Tensile Strength, Yield | >= 9.80 MPa | >= 1420 psi | |
Kazanorgsintez 102-11K Cable Composition Based on Low Density Polyethylene Production Method: Produced in the form of pellets (natural or black colored) on the bases of basic 10204-003, 15303-003, 15313-003. Application: Designed to apply isolation, cable covers and ca.. |
|||
Tensile Strength, Yield | >= 9.80 MPa | >= 1420 psi | |
Kazanorgsintez 102-12K Cable Composition Based on Low Density Polyethylene Production Method: Produced in the form of pellets (natural or black colored) on the bases of basic 10204-003, 15303-003, 15313-003. Application: Designed to apply isolation, cable covers and ca.. |
|||
Tensile Strength, Yield | >= 9.80 MPa | >= 1420 psi | |
Kazanorgsintez 153-03K Cable Composition Based on Low Density Polyethylene Production Method: Produced in the form of pellets (natural or black colored) on the bases of basic 10204-003, 15303-003, 15313-003. Application: Designed to apply isolation, cable covers and ca.. |
|||
Tensile Strength, Yield | >= 9.80 MPa | >= 1420 psi | |
Kazanorgsintez 153-05K Cable Composition Based on Low Density Polyethylene Production Method: Produced in the form of pellets (natural or black colored) on the bases of basic 10204-003, 15303-003, 15313-003. Application: Designed to apply isolation, cable covers and ca.. |
|||
Tensile Strength, Yield | >= 9.80 MPa | >= 1420 psi | |
Kazanorgsintez 153-10K Polyethylene Composition for Cable Industry Production Method: Composition is achieved on the basis of high pressure polyethylene (low density) and low pressure (high density) with stabilizers and other additives. Application: Composition.. |
|||
Tensile Strength, Yield | >= 9.80 MPa | >= 1420 psi | |
Kazanorgsintez 153-12K Cable Composition Based on Low Density Polyethylene Production Method: Produced in the form of pellets (natural or black colored) on the bases of basic 10204-003, 15303-003, 15313-003. Application: Designed to apply isolation, cable covers and ca.. |
|||
Tensile Strength, Yield | >= 9.80 MPa | >= 1420 psi | |
Kazanorgsintez 15313-003 High Pressure Polyethylene Production Method: HDPE is produced by high pressure ethylene polymerization in tubular reactors. Application: Intended for production of bags, pipes, fittings, articles designed for food contac.. |
|||
Tensile Strength, Yield | >= 9.80 MPa | >= 1420 psi | |
Kazanorgsintez 175-76 Film Grade Composition of High Density Polyethylene Production Method: Based on polyethylene grades 10803-20, 15803-20, 15813-020,17504-006. Application: Designed for packing manufacture for milk and milk products.Information Provided by Kazanorg.. |
|||
Tensile Strength, Yield | 9.80 MPa @Strain 100 % |
1420 psi @Strain 100 % |
ASTM D412 |
LG Chemical KEYFLEX TO-1045D Thermoplastic Olefin for Injection Molding, 45D Hardness KEYFLEX resins, thermoplastic elastomers divided by polyester and polyolefin type, have been developed by LG`s own polymerization and compounding technology. They display the flexibility of rubber .. |
|||
Tensile Strength, Yield | 9.79 MPa | 1420 psi | AVG Stress at Elongation M100; ASTM D412 Method A |
Seals Eastern 7344 Highly Saturated Nitrile Rubber HNBR for Oil & Gas serviceInformation provided by Seals Eastern, Inc. |
|||
Tensile Strength, Yield | 9.80 MPa | 1420 psi | 500 mm/min; GOST 11262 |
Sibur 15303-003 Low Density Polyethylene For production of films and film articles, including thermoset films, thin films, food contact grade films
(including tight packing), general-purpose films, and bags. |
|||
Tensile Strength, Yield | 9.79 MPa | 1420 psi | 9.8 in/min; ASTM D638 |
Teknor Apex Sinvicomp SFW 9000 Polyvinyl Chloride, Flexible Availability: Asia Pacific Uses: Footwear; General Purpose Forms: Pellets Processing Method: Injection MoldingInformation Provided by Teknor Apex |
|||
Tensile Strength, Yield | 9.79 MPa | 1420 psi | 20 in/min; ASTM D638 |
Teknor Apex Sinvicomp SHM 4200 Polyvinyl Chloride, Flexible Availability: Asia Pacific Features: Ethylene Oxide Sterilizable Uses: Medical/Healthcare Applications Forms: Pellets Processing Method: Injection MoldingInformation Provided by Teknor Apex |
|||
Tensile Strength, Yield | 9.79 MPa | 1420 psi | 20 in/min; ASTM D638 |
Teknor Apex Sinvicomp SMG 9000 Polyvinyl Chloride, Flexible Availability: Asia Pacific Features: Food Contact Acceptable; Non-Toxic Uses: Toys Forms: Pellets Processing Method: Injection MoldingInformation Provided by Teknor Apex |
|||
Tensile Strength, Yield | 9.81 MPa | 1420 psi | at 100% elongation; ASTM D412 |
Lubrizol Estane® S392A Thermoplastic Polyurethane Type: Estane® S392A is a Shore 93A, polyester based thermoplastic polyurethane (TPU) with excellent transparency. FDA approved (21 CFR 177.2600, 177.1680).Uses: Injection Molding, Extrusion, Blow .. |
|||
Tensile Strength, Yield | 9.79 MPa | 1420 psi | 9.8 in/min; ASTM D638 |
Teknor Apex Sinvicomp SPF 8020 Polyvinyl Chloride, Flexible Availability: Asia Pacific Features: Good Stiffness Uses: Gaskets; Profiles; Seals Forms: Pellets Processing Method: ExtrusionInformation Provided by Teknor Apex |
|||
Tensile Strength, Yield | 9.80 MPa | 1420 psi | Elastic Limit |
Wolf Kunststoff ZEDEX® ZX-550 A5L Polymer Alloy Main Characteristics: Strong anti-adhesive; Low creep; Weather resistant; No water absorption; Good machinability; Strongly viscoelastic; Stress resistantApplications: Chemical Engineering; Laborato.. |
|||
Tensile Strength, Yield | 9.79 MPa | 1420 psi | heat aged one week at 300ºF |
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer with 80 PHR N330 (HAF) Black MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c.. |
|||
Tensile Strength, Yield | 9.81 MPa | 1420 psi | at 300% elongation; ASTM D412 |
Lubrizol Estane® CS185A Thermoplastic Polyurethane Type: Estane® CS185A is a Shore 85A, polyester grade, calendering processible thermoplastic polyurethane (TPU). FDA approved (21 CFR 177.2600, 177.1680).Uses: Calendering, Molt roll processing.Inf.. |
|||
Tensile Strength, Yield | 9.81 MPa | 1420 psi | at 100% elongation; ASTM D412 |
Lubrizol Estane® CS195A Thermoplastic Polyurethane Type: Estane® CS195A is a Shore 95A, polyester grade, calendering processible thermoplastic polyurethane (TPU). FDA approved (21 CFR 177.2600, 177.1680).Uses: Calendering, Molt roll processing.Inf.. |
|||
Tensile Strength, Yield | 9.81 MPa | 1420 psi | at 300% elongation; ASTM D412 |
Lubrizol Estane® R185A Thermoplastic Polyurethane Type: Estane® R185A is a Shore 85A, polyether type thermoplastic polyurethane (TPU). FDA approved (21 CFR 177.2600, 177.1680).Uses: Injection Molding, Extrusion.Availability: AsiaInformation Provi.. |
|||
Tensile Strength, Yield | 9.81 MPa | 1420 psi | at 100% elongation; ASTM D412 |
Lubrizol Estane® R190A Thermoplastic Polyurethane Type: Estane® R190A is a Shore 93A, polyether type thermoplastic polyurethane (TPU). FDA approved (21 CFR 177.2600, 177.1680).Uses: Injection Molding, Extrusion.Availability: AsiaInformation Provi.. |
|||
Tensile Strength, Yield | 9.79 MPa | 1420 psi | 20 in/min; ASTM D638 |
Teknor Apex Sinvicomp SMG 10500 Polyvinyl Chloride, Flexible Availability: Asia Pacific Features: Food Contact Acceptable; Non-Toxic Uses: Toys Forms: Pellets Processing Method: Injection MoldingInformation Provided by Teknor Apex |
|||
Tensile Strength, Yield | 9.80 MPa | 1420 psi | Molded property |
Dow Primacor® 1321 Ethylene Acrylic Acid (EAA) PRIMACOR® 1321 polymer is an EAA copolymer (% comonomer 6.5) for blown and cast films. Its outstanding properties include, excellent sealability, toughness, adhesion and tear resistance. PRIMACOR 1.. |
|||
Tensile Strength, Yield | 9.79 MPa | 1420 psi | heat aged one week at 300ºF |
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer with 80 PHR N330 (HAF) Black MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c.. |