Karina E-844-10/219-Y-ERYM White PVC Compound

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Extruded
Manufacturer Karina Indústria e Comércio de Plásticos
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Karina E-844-10/219-Y-ERYM White PVC Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Tin stabilized PVC compound, recommended for extrusion of profiles for general applications. It is supplied in pellet form and should be processed at the temperature range of 170°C to 190°C.Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Physical Properties Metric English Comments
Specific Gravity 1.44 - 1.50 g/cc
1.44 - 1.50 g/cc
ASTM D 792
ASTM Color -5.07 - -3.47
-5.07 - -3.47
Color B, ME 12
-1.70 - -0.100
-1.70 - -0.100
Color A, ME 12
89.59 - 91.19
89.59 - 91.19
Color L, ME 12
Mechanical Properties Metric English Comments
Hardness, Shore D 78 - 82

@Time 15.0 sec
78 - 82

@Time 0.00417 hour
ASTM D 2240
Tensile Strength >= 39.2 MPa
>= 5690 psi
ASTM D 638
Elongation at Break >= 70 %
>= 70 %
ASTM D 638
Izod Impact, Notched >= 1.34 J/cm
>= 2.51 ft-lb/in
Method A; ASTM D 256
Thermal Properties Metric English Comments
Vicat Softening Point >= 81.0 °C
>= 178 °F
ASTM D 1525
Heat Distortion Temperature >= 75.0 °C
>= 167 °F
ASTM D 648
Descriptive Properties Value Comments
Application General Purpose Profiles
Torque 35
ME 37