Polymer Property : Heat Distortion Temperature = 75.0 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Heat Distortion Temperature >= 75.0 °C
>= 167 °F
ASTM D 648
Karina E-844-10/219-Y-ERYM White PVC Compound
Tin stabilized PVC compound, recommended for extrusion of profiles for general applications. It is supplied in pellet form and should be processed at the temperature range of 170°C to 190°C.I..
Heat Distortion Temperature >= 75.0 °C
>= 167 °F
ASTM D 648
Karina E-854-10/390-B-ERYB White PVC Compound
Heavy metal free PVC compound recommended for extrusion of profiles.Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Heat Distortion Temperature 75.0 °C
167 °F
ASTM D648
IRPC Polimaxx Polene 3325M Polypropylene Random Copolymer
CHARACTERISTICS: GOOD EXTRUDABILITY, GOOD SEALABLE CONTAINS SLIP AND ANTIBLOCK ADDITIVES APPLICATIONS: CAST FILM EXTRUSION CPP FILM FOR LAMINATE , CPP FILM FOR PACKAGINGS
Heat Distortion Temperature >= 75.0 °C
>= 167 °F
ASTM D 648
Karina E 830-10/150-Y-ERYB-LMP White PVC Compound
Heavy metal free PVC compound recommended for extrusion of furniture profiles.Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Heat Distortion Temperature >= 75.0 °C
>= 167 °F
ASTM D 648
Karina E 830-35/1-Y-ERYB-LMP Ivory PVC Compound
Heavy metal free PVC compound recommended for extrusion of furniture profiles/.p>Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Heat Distortion Temperature >= 75.0 °C
>= 167 °F
ASTM D 648
Karina E 832-35/1-Y-ERA-LMP Ivory PVC Compound
Heavy metal free PVC compound recommended for extrusion of furniture profiles.Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Heat Distortion Temperature >= 75.0 °C
>= 167 °F
ASTM D 648
Karina E 832-35/1-Y-ERYB-LMP Ivory PVC Compound
Heavy metal free PVC compound recommended for extrusion of furniture profiles.Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Heat Distortion Temperature >= 75.0 °C
>= 167 °F
ASTM D 648
Karina E 834-35/1-Y-ERA-LMP Ivory PVC Compound
Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Heat Distortion Temperature >= 75.0 °C
>= 167 °F
ASTM D 648
Karina E 836-10/185-ERYB White PVC Compound
Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Heat Distortion Temperature >= 75.0 °C
>= 167 °F
ASTM D648
Karina E 854-10/150-A-ERYB White PVC Compound
Heavy metal free PVC compound recommended for extrusion of furniture profiles.Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Heat Distortion Temperature >= 75.0 °C
>= 167 °F
ASTM D 648
Karina E 854-10/150-ERYB White PVC Compound
Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Heat Distortion Temperature >= 75.0 °C
>= 167 °F
ASTM D 648
Karina E 854-10/185-ERYB White PVC Compound
Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Heat Distortion Temperature >= 75.0 °C
>= 167 °F
ASTM D 648
Karina E 854-35/1-A-ERYB Ivory PVC Compound
Heavy metal free PVC compound recommended for extrusion of furniture profiles.Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Heat Distortion Temperature >= 75.0 °C
>= 167 °F
ASTM D 648
Karina E 854-35/1-Y-ERYB Ivory PVC Compound
Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Heat Distortion Temperature >= 75.0 °C
>= 167 °F
ASTM D 648
Karina E 855-10/150-ERYB-PO White PVC Compound
Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Heat Distortion Temperature 75.0 °C
167 °F
ASTM D648
Wanshijie APET Sheet
APET sheet is one of the earliest plastic sheets our company develops and produces. It has excellent air-tightness, durability, chemical resistance and transparency. When burnt, it will not produce ..
Heat Distortion Temperature >= 75.0 °C
>= 167 °F
ASTM D 648
Karina E 841-08/184-A-ERYB Beige PVC Compound
Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Heat Distortion Temperature >= 75.0 °C
>= 167 °F
ASTM D 648
Karina E 841-08/184-Y-ERYB Beige PVC Compound
Information provided by Karina Indústria e Comércio de Plásticos Ltda.