Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Strength = 39.2 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength >= 39.2 MPa
>= 5690 psi
ASTM D 638
Karina E-844-10/219-Y-ERYM White PVC Compound
Tin stabilized PVC compound, recommended for extrusion of profiles for general applications. It is supplied in pellet form and should be processed at the temperature range of 170°C to 190°C.I..
Tensile Strength 39.2 MPa
5690 psi
ASTM D638
Gromax CCP PBT 1100-220S
Product Description: PBT unreinforced and impact-modified injection molding grade. Characteristics:Low warp age, high toughness and excellent dimensional stabilityExcellent glossy surface and less-g..
Tensile Strength >= 39.2 MPa
>= 5690 psi
ASTM D 638
Karina 760-35/1-IS-SD Ivory PVC Compound
PVC compound for extrusion of monofilament.Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Tensile Strength >= 39.2 MPa
>= 5690 psi
ASTM D 638
Karina 804-02/39-Y-RTC Blue PVC Compound
Flame retardant PVC compound recommended for electrical conduit extrusion.Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Tensile Strength >= 39.2 MPa
>= 5690 psi
ASTM D 638
Karina 804-02/69-Y-RTC Yellow PVC Compound
Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Tensile Strength >= 39.2 MPa
>= 5690 psi
ASTM D 638
Karina 804-48/1-CRE Black PVC Compound
Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Tensile Strength >= 39.2 MPa
>= 5690 psi
ASTM D 638
Karina 806-10/42-B-RT-PO White PVC Compound
PVC powder compound, recommended for extrusion in twin screw extruder of sewer pipes.Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Tensile Strength >= 39.2 MPa
>= 5690 psi
ASTM D 638
Karina 806-48/1-BY-ERYB Black PVC Compound
Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Tensile Strength >= 39.2 MPa
>= 5690 psi
ASTM D 638
Karina 811-10/23-A-ERYB-PO White PVC Compound
PVC powder compound, recommended for extrusion in twin screw extruder of sewer pipes.Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Tensile Strength >= 39.2 MPa
>= 5690 psi
ASTM D 638
Karina 818-10/121-AY-ERYB White PVC Compound
Lead stabilized PVC compound, recommended for extrusion of profiles for general applications. It is supplied in pellet form and should be processed at the temperature range of 170°C to 190°C...
Tensile Strength >= 39.2 MPa
>= 5690 psi
ASTM D 638
Karina 828-28/14-AY-ERYB Ice (Light Gray) PVC Compound
Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Tensile Strength >= 39.2 MPa
>= 5690 psi
ASTM D 638
Karina 834-48/1-A-ERM-LMP Black PVC Compound
Heavy metal free PVC compound recommended for extrusion of automotive profiles.Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Tensile Strength >= 39.2 MPa
>= 5690 psi
ASTM D 638
Karina 850-10/99-Y-ERYB White PVC Compound
Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Tensile Strength >= 39.2 MPa
>= 5690 psi
ASTM D 638
Karina 851-10/127-Y-ERYB-AS-PO White PVC Compound
Weather resistant PVC powder compound recommended for extrusion in twin screw extruder of window and door profiles.Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Tensile Strength >= 39.2 MPa
>= 5690 psi
ASTM D 638
Karina E 74/240-D-IS-SD-TR Compound PVC Crystal
Films, laminated shrinkInformation provided by Karina Indústria e Comércio de Plásticos Ltda.
Tensile Strength >= 39.2 MPa
>= 5690 psi
ASTM D 638
Karina E 76/205-IS-SD-TR Crystal PVC Compound
Crystal PVC compound recommended for sleeves.Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Tensile Strength >= 39.2 MPa
>= 5690 psi
ASTM D 638
Karina E 811-10/184-Y-ERYB White PVC Compound
Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Tensile Strength >= 39.2 MPa
>= 5690 psi
ASTM D 638
Karina E 813-35/1-DY-SN-ERYB Compound PVC Ivory
Ivory PVC compound recommended for extrusion of profiles developed for Teknaform Canada.Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Tensile Strength >= 39.2 MPa
>= 5690 psi
ASTM D 638
Karina E 813-35/1-Y-SN-ERYB Ivory PVC Compound
Tin stabilized PVC compound recommended for extrusion of interior furnishing boards and profiles. Developed for Teknaform Canada.Information provided by Karina Indústria e Comércio de Plás..
Tensile Strength >= 39.2 MPa
>= 5690 psi
ASTM D 638
Karina E 828-08/497-Y-RT Beige PVC Compound
Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Tensile Strength >= 39.2 MPa
>= 5690 psi
ASTM D 638
Karina E 828-18/569-Y-RT Gray PVC Compound
Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Tensile Strength >= 39.2 MPa
>= 5690 psi
ASTM D 638
Karina E 828-48/27-Y-RT Black PVC Compound
Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Tensile Strength >= 39.2 MPa
>= 5690 psi
ASTM D 638
Karina E 832-10/84-Y-ERM White PVC Compound
Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Tensile Strength >= 39.2 MPa
>= 5690 psi
ASTM D 638
Karina E 835-18/115-C-ERYB Gray PVC Compound
Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Tensile Strength >= 39.2 MPa
>= 5690 psi
ASTM D 638
Karina E 835-35/1-ERYB-AS Ivory PVC Compound
Rigid ivory PVC compound with anti-UV protection, developed for extrusion profile under 8700x0220 sample analysis.Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Tensile Strength >= 39.2 MPa
>= 5690 psi
ASTM D 638
Karina E 838-10/182-ERYB White PVC Compound
Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Tensile Strength >= 39.2 MPa
>= 5690 psi
ASTM D 638
Karina E 854-10/144-ERYM White PVC Compound
Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Tensile Strength >= 39.2 MPa
>= 5690 psi
ASTM D 638
Karina 753-35/1-Y-IS-SD Ivory PVC Compound
Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Tensile Strength 39.2 MPa
5690 psi
Taiwan Sheen Soon Sheenthane® A9550 Thermoplastic Polyurethane Elastomer
Thermoplastic polyurethane elastomer for injection moldingPolyether gradeInformation provided by Taiwan Sheen Soon Co., LTD.
Tensile Strength >= 39.2 MPa
>= 5690 psi
ASTM D 638
Karina E 842-18/106-Y-RT-POWDER Compound PVC Gray
Rigid powder PVC compound recommended for extrusion of profiles.Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Copyright © lookpolymers.com All Rights Reserved