Isoflon Tisoflon® 5 AD Polytetrafluoroethylene Coated Glass Fabric

Category Ceramic , Glass , Glass Fiber , Polymer , Thermoplastic , Fluoropolymer , PTFE , Polytetrafluoroethylene (PTFE), Glass Filled, Molded
Manufacturer Isoflon
Trade Name Tisoflon®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Isoflon Tisoflon® 5 AD Polytetrafluoroethylene Coated Glass Fabric.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PTFE coated glass fabric one side adhesive TISOFLON® - Standard gradeInformation provided by Isoflon.
Physical Properties Metric English Comments
Thickness 120 microns
4.72 mil
Coating Weight 250 g/m²
156 lb/ream
entire thickness; NF EN ISO 2286.2
Mechanical Properties Metric English Comments
Tear Strength 23.0 - 26.0 kN/m
131 - 148 pli
NF EN ISO 1421
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 260 °C
500 °F
Minimum Service Temperature, Air -150 °C
-238 °F
Electrical Properties Metric English Comments
Dielectric Strength 30.8 kV/mm
782 kV/in
NF EN 60243.1
Descriptive Properties Value Comments
PTFE Content (%) 58