Polymer Property : Tear Strength = 148 pli Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tear Strength 23.0 - 26.0 kN/m
131 - 148 pli
NF EN ISO 1421
Isoflon Tisoflon® 5G Polytetrafluoroethylene & Graphite Coated Glass Fabric
PTFE + Graphite coated glass fabric TISOFLON® - Black anti-staticInformation provided by Isoflon.
Tear Strength 23.0 - 26.0 kN/m
131 - 148 pli
NF EN ISO 1421
Isoflon Tisoflon® 6 AD EXTRA SMOOTH Polytetrafluoroethylene Coated Glass Fabric
PTFE coated glass fabric one side adhesive TISOFLON® - Standard gradeInformation provided by Isoflon.
Tear Strength 23.0 - 26.0 kN/m
131 - 148 pli
NF EN ISO 1421
Isoflon Tisoflon® 6G EXTRA SMOOTH QUALITY Polytetrafluoroethylene & Graphite Coated Glass Fabric
PTFE + Graphite coated glass fabric TISOFLON® - Black anti-staticInformation provided by Isoflon.
Tear Strength 23.0 - 26.0 kN/m
131 - 148 pli
NF EN ISO 1421
Isoflon Tisoflon® 5 AD Polytetrafluoroethylene Coated Glass Fabric
PTFE coated glass fabric one side adhesive TISOFLON® - Standard gradeInformation provided by Isoflon.