Iran Petrochemical (PCC) LL 18XF5 N Linear Low Density Polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE) , LLDPE , Linear Low Density Polyethylene (LLDPE), Blow Molding Grade
Manufacturer Iran Petrochemical Commercial Co. (PCC)
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Iran Petrochemical (PCC) LL 18XF5 N Linear Low Density Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LL 18XF5 N is a terpolymer of ethylene, propylene and butene-1 for high film strength applications, especially heavy duty shipping sacks, ice bags, frozen food bags, potato bags, and agriculture films. Goods produced from this grade have outstanding toughness, excellent puncture resistance, good heat sealing behavior and excellent machinability on conversion lines.Information provided by Iran Petrochemical Commercial Co.
Physical Properties Metric English Comments
Density 0.920 g/cc
0.0332 lb/in³
ASTM D1505
Melt Flow 0.50 g/10 min
0.50 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 11.0 MPa
1600 psi
ASTM D882
Film Tensile Strength at Yield, TD 10.0 MPa
1450 psi
ASTM D882
Film Elongation at Break, MD 600 %
600 %
ASTM D882
Film Elongation at Break, TD 750 %
750 %
ASTM D882
Elmendorf Tear Strength MD 240 g
240 g
ASTM D1922
Elmendorf Tear Strength TD 400 g
400 g
ASTM D1922
Dart Drop Test 125 g
0.276 lb
ASTM D1709
Film Tensile Strength at Break, MD 40.0 MPa
5800 psi
ASTM D882
Film Tensile Strength at Break, TD 35.0 MPa
5080 psi
ASTM D882
Optical Properties Metric English Comments
Haze 30 %
30 %
ASTM D1003
Gloss 25 %
25 %
ASTM D2457