Polymer Property : Elmendorf Tear Strength TD = 400 g Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Elmendorf Tear Strength TD 400 g
400 g
ASTM D1922
SABIC 218B Linear Low Density Polyethylene for Cast Film
Product Description: 218B is a Linear Low Density Polyethylene grade designed to provide easy processability and specially formulated for optimum thermal stability at high processing temperatures u..
Elmendorf Tear Strength TD 400 g
400 g
ASTM D1922
SABIC 518N Linear Low Density Polyethylene for Blown Film
Product Description: 548N is a fractional melt index Linear Low Density Polyethylene grade suitable for high strength packaging applications. Films produced using this resin yield outstanding toug..
Elmendorf Tear Strength TD 400 g
400 g
ASTM D1922
LyondellBasell Alathon® M6010SB High Density Polyethylene, MMW Film Grade
Alathon M6010SB is a medium molecular weight high density polyethylene homopolymer for use in blown film applications. Typical applications include those with low WVTR requirements. Regulatory Statu..
Elmendorf Tear Strength TD 400 g
400 g
ASTM D1922
LyondellBasell Petrothene® GA502022 Linear Low Density Polyethylene
ApplicationsThe PETROTHENE GA 502 series of resins are pelletized linear low density polyethylene for film extrusion applications requiring excellent drawdown and toughness. These pelletized produc..
Elmendorf Tear Strength TD 400 g
400 g
ASTM D1922
LyondellBasell Petrothene® GA502024 Linear Low Density Polyethylene
ApplicationsThe PETROTHENE GA 502 series of resins are pelletized linear low density polyethylene for film extrusion applications requiring excellent drawdown and toughness. These pelletized produc..
Elmendorf Tear Strength TD 400 g
400 g
ASTM D1922
Iran Petrochemical (PCC) LL 18XF5 N Linear Low Density Polyethylene
LL 18XF5 N is a terpolymer of ethylene, propylene and butene-1 for high film strength applications, especially heavy duty shipping sacks, ice bags, frozen food bags, potato bags, and agriculture fil..
Elmendorf Tear Strength TD 400 g
400 g
ASTM D1922
LyondellBasell Petrothene® GA502023 Linear Low Density Polyethylene
ApplicationsThe PETROTHENE GA 502 series of resins are pelletized linear low density polyethylene for film extrusion applications requiring excellent drawdown and toughness. These pelletized produc..
Elmendorf Tear Strength TD 400 g
400 g
ASTM D1922
Formosa Plastics Formolene® L42009F Film (Butene Grade) LLDPE
Extra High Molecular Weight Hexene Copolymer Formolene® L42009F is a general-purpose film grade linear low density made using gas-phase technology. The resin exhibits excellent toughness and streng..
Elmendorf Tear Strength TD 400 g
400 g
ASTM D1922
ExxonMobil Exceed™ 2018CA Metallocene Polyethylene Resin (European Grade)
Product Description: Exceed 2018CA is a metallocene ethylene-hexene copolymer. The higher melt index makes this polymer ideally suited for blending into LDPE rich films as well as skin layer in coex..
Elmendorf Tear Strength TD 400 g
400 g
ASTM D1922
ExxonMobil LLDPE LL 1001X26 Linear Low Density Polyethylene Resin
Product Description: LL 1001 are butane LLDPE blown film resins having good draw down. Films made from LL 1001 resins exhibit good tensile and toughness properties. Availability: Latin America, Nort..
Elmendorf Tear Strength TD 400 g
400 g
ASTM D1922
ExxonMobil LLDPE LL 1001X31 Linear Low Density Polyethylene Resin
Product Description: LL 1001 are butane LLDPE blown film resins having good draw down. Films made from LL 1001 resins exhibit good tensile and toughness properties. Availability: Latin America, Nort..
Elmendorf Tear Strength TD 400 g
400 g
ASTM D1922
ExxonMobil LLDPE LL 1001X72 Linear Low Density Polyethylene Resin
Product Description: LL 1001 are butane LLDPE blown film resins having good draw down. Films made from LL 1001 resins exhibit good tensile and toughness properties. Availability: Latin America, Nort..
Elmendorf Tear Strength TD 400 g
400 g
ASTM D1922
ExxonMobil LLDPE LL 1001X74 Linear Low Density Polyethylene Resin
Product Description: LL 1001 are butane LLDPE blown film resins having good draw down. Films made from LL 1001 resins exhibit good tensile and toughness properties. Availability: Latin America, Nort..
Elmendorf Tear Strength TD 400 g
400 g
ASTM D1922
ExxonMobil LLDPE LL 1001X76 Linear Low Density Polyethylene Resin
Product Description: LL 1001 are butane LLDPE blown film resins having good draw down. Films made from LL 1001 resins exhibit good tensile and toughness properties. Availability: Latin America, Nort..
Elmendorf Tear Strength TD 400 g
400 g
ASTM D1922
Dow FLEXOMER™ ETS-9066 NT 7, 0.8 mil Very Low Density Polyethylene (VLDPE) Resin
FLEXOMER™ ETS-9066 NT 7 is intended for use in single of multi-layer blown-film constructions or thick sheets. Films extruded from ETS-9064 NT 7 have a high tear strength, high impact strength, an..
Elmendorf Tear Strength TD 400 g
400 g
Dow Primacor® 1410 Ethylene Acrylic Acid (EAA)
Film properties below based on a film thickness of 60 µm. Data provided by Dow Chemical.
Elmendorf Tear Strength TD 400 g
400 g
ASTM-D1922
Braskem FG31 LLDPE Blown Film Extrusion Polyethylene Copolymer
FG31 is a linear low-density polyethylene, copolymer of butene-1, produced by the solution process. It was developed for blown film extrusion in blends with polyethylene. Films obtained with this pr..
Elmendorf Tear Strength TD 400 g
400 g
gF; ASTM D1922
Braskem Green PE SLL118/21 Blow Film Extrusion and Cast Film Extrusion Linear Low Density Polyethylene
Description: SLL118/21 is a LLDPE Butene copolymer produced by Braskem. It is a general purpose product that shows a good processing performance balanced with good optical and mechanical properties ..
Elmendorf Tear Strength TD 400 g
400 g
ASTM-D1922
Braskem LF118 LLDPE Blown Film Extrusion Polyethylene Copolymer
LF118 is a linear low-density polyethylene, copolymer of butene-1, produced by the gas phase process. It is developed for blown film extrusion in blends with polyethylene. Films obtained with this p..
Elmendorf Tear Strength TD 400 g
400 g
gF; ASTM D1922
Braskem LL118/21 Blown Film Extrusion Linear Low Density Polyethylene
Description: LL118/21 is a LLDPE Butene copolymer produced by Braskem. It is a general purpose product that shows a good processing performance balanced with good optical and mechanical properties a..
Elmendorf Tear Strength TD 400 g
400 g
ASTM D1922
Total Lumicene® mPE M 3410 EP Metallocene Medium Density Film Resin  (Unverified Data**)
Polyethylene: Metallocene Medium Density Film ResinCharacteristics:Outstanding clarity and glossExcellent bubble stabilityHigh StiffnessGood puncture resistanceGood tear strengthGood heat sealing p..
Elmendorf Tear Strength TD 400 - 890 g
400 - 890 g
Average value: 535 g Grade Count:11
Overview of materials for Linear Low Density Polyethylene (LLDPE), Blow Molding Grade
This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE), Blow Molding Grade". Each property range of values reported is ..
Elmendorf Tear Strength TD 400 g
400 g
ASTM D1922
ExxonMobil Exceed™ 3527PA Metallocene Polyethylene Resin
Product Description: Exceed 3527PA is a metallocene ethylene-hexene copolymer. Films made from Exceed 3527PA have high modulus and outstanding tensile, impact and puncture resistance properties. The..
Elmendorf Tear Strength TD 400 g
400 g
gF; ASTM D1922
Braskem LF0720/20AF Blown Film Extrusion Linear Low Density Polyethylene
Description: LF0720/21AF is a LLDPE Butene copolymer produced using Unipol process technology. It shows excellent optical properties associated with good balance of mechanical properties, processing..