Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength MD | 240 g | 240 g | ASTM D1922 |
Iran Petrochemical (PCC) LL 18XF5 N Linear Low Density Polyethylene LL 18XF5 N is a terpolymer of ethylene, propylene and butene-1 for high film strength applications, especially heavy duty shipping sacks, ice bags, frozen food bags, potato bags, and agriculture fil.. |
|||
Elmendorf Tear Strength MD | 240 g | 240 g | ASTM D1922 |
ExxonMobil Escorene™ LD 723.28 Cast Ethylene Vinyl Acetate Copolymer Product Description: Escorene Ultra UL 723.28 is a high VA extrusion coating resin, which provides outstanding heat sealability and high clarity. LD 723.28 has a good balance of drawabilty and neck-.. |
|||
Elmendorf Tear Strength MD | 240 g | 240 g | ASTM D1922 |
ExxonMobil LD 313.NF Blown Film Resin LD 313.NF is a 3 wt% vinyl acetate copolymer. The vinyl acetate content of this resin provides good heat sealing and good cold temperature toughness when compared to LDPE homopolymers.Information pr.. |
|||
Elmendorf Tear Strength MD | 240 g | 240 g | |
Dow DOWLEX™ 2049 Linear Low Density Polyethylene, Food Grade DOWLEX® 2049 Polyethylene resin offers excellent tear strength, medium stiffness, outstanding toughness and puncture resistance for films used in food contact applications. When used unmodified and.. |
|||
Elmendorf Tear Strength MD | 240 g | 240 g | gF; ASTM D1922 |
Braskem Flexus® 9200 Blown Film Extrusion Polyethylene Description: Flexus 9200 is a LLDPE hexene copolymer produced through metallocene catalyst which presents excellent impact and puncture strength, beyond a differential sealing performance comparing .. |
|||
Elmendorf Tear Strength MD | 240 g | 240 g | gF; ASTM D1922 |
Braskem Green PE SLH218 Blow Film Extrusion and Cast Film Extrusion Linear Low Density Polyethylene Description: SLH218 is a LLDPE Hexene copolymer produced by Braskem. It shows a good balance between optical properties, mechanical properties (Mainly stretchability), sealability and processability.. |
|||
Elmendorf Tear Strength MD | 240 g | 240 g | gF; ASTM D1922 |
Braskem LH218 Cast Film Extrusion Linear Low Density Polyethylene Description: LH218 is a LLDPE Hexene copolymer produced by Braskem. It shows a good balance between optical properties, mechanical properties (Mainly stretchability), sealability and processability... |