Ineos J50-200-178 HDPE

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Injection Molded
Manufacturer Ineos Olefins & Polymers USA
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ineos J50-200-178 HDPE.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A high density polyethylene copolymer. It has a narrow molecular weight distribution and is intended for the molding of screw caps dedicated to the packaging of carbonated beverages. This material meets the Food and Drug Administration requirements of 21CFR 177.1520.
Physical Properties Metric English Comments
Density 0.952 g/cc
0.0344 lb/in³
ASTM D4883
Environmental Stress Crack Resistance 12 hour
12 hour
Condition B, 10%; ASTM D1693
Melt Flow 2.2 g/10 min

@Load 2.16 kg,
Temperature 190 °C
2.2 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 65
65
ASTM D2240
Tensile Strength, Yield 26.9 MPa
3900 psi
2 in/min.; ASTM D638
Elongation at Break >= 800 %
>= 800 %
2 in/min.; ASTM D638
Flexural Modulus 1.276 GPa
185.1 ksi
Tangent-Method 1; ASTM D790
Izod Impact, Notched 1.23 J/cm
2.30 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 77.0 °C
171 °F
ASTM D648
Vicat Softening Point 131 °C
268 °F
ASTM D1525
Brittleness Temperature <= -75.0 °C
<= -103 °F
ASTM D 746
Descriptive Properties Value Comments
Process Injection