Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 26.9 MPa | 3900 psi | ASTM D638 |
Multibase Multi-Pro® 3019 CXUW Polypropylene Calcium Carbonate Filler, 30% by weight.Features:Gloss, High Impact Resistance, GoodUV Resistance, Good Forms:PelletsProcessing Methods:Injection MoldingUses:FurnitureLawn EquipmentInformation prov.. |
|||
Tensile Strength, Yield | 26.9 MPa | 3900 psi | 2 in per min; ASTM D638 |
Network Polymers NPP 25-0802 Description: Copolymer PolypropyleneInformation provided by Network Polymers Inc. |
|||
Tensile Strength, Yield | 26.9 MPa | 3900 psi | ASTM D638 |
Petromont 5000 High Density Polyethylene Resin Petromont HDPE 5000 is a high density polyethylene copolymer resin produced using the UNIPOL™ Process. This resin is intended for use in prime sheet and thermoforming applications such as arena boa.. |
|||
Tensile Strength, Yield | >= 26.9 MPa | >= 3900 psi | ASTM D 638 type IV |
Total Finathene® 5302 HDPE drain tile, corrugated pipe resin
(discontinued **) Applications: corrugated pipe, storm and sanitary sewers, drainage systemsInformation provided provided by Total Petrochemicals.Total Petrochemicals includes former Fina and Atofina plastics produc.. |
|||
Tensile Strength, Yield | 26.9 MPa | 3900 psi | ASTM D638 |
LyondellBasell Alathon® M6080WC High Density Polyethylene ApplicationsALATHON M 6080WC is a natural, high density, polyethylene homopolymer resin with a narrow molecular weight distribution formulated for use as primary insulation for coaxial and control c.. |
|||
Tensile Strength, Yield | 26.9 MPa | 3900 psi | ASTM D638 |
M. Holland Company CP850 Polypropylene Impact Copolymer Impact copolymerFast production cycleHigh flowHigh stiffnessApplications: ContainersHousehold goodsThin-walled parts |
|||
Tensile Strength, Yield | 26.9 MPa | 3900 psi | 2 in/min; ASTM D638 |
Ineos T50-500-171 Polyethylene Copolymer This is a high density polyethylene copolymer having a narrow molecular weight distribution. It is intended for injection molding applications where a good balance of processability and end-use pro.. |
|||
Tensile Strength, Yield | 26.9 MPa | 3900 psi | 2 in/min; ASTM D638 |
Ineos T50-800-01 Polyethylene Copolymer This is a high density polyethylene copolymer having a narrow molecular weight distribution. It is intended for injection molding applications where a good balance of processability and end-use pro.. |
|||
Tensile Strength, Yield | 26.9 MPa | 3900 psi | ASTM D638 |
LTL Color Compounds ColorRxâ„¢ PP2-1002AF Food Grade Polypropylene Random Copolymer An approx. 10 melt Polypropylene random copolymer with FDA food contact approval and antimicrobial protection.All information provided by LTL Color Compounders, Inc. |
|||
Tensile Strength, Yield | 26.9 MPa | 3900 psi | ASTM D638 |
LTL Color Compounds ColorRxâ„¢ PP2-1005ARX Biocompatible, Antimicrobial Polypropylene Random Copolymer A biocompatible approx. 10 melt Polypropylene random copolymer for healthcare applications, containing a high level of antimicrobial protection for FDA regulated medical devices.All information prov.. |
|||
Tensile Strength, Yield | 26.9 MPa | 3900 psi | 2 in/min (50 mm/min); ASTM D-638 |
Ineos R01A-01 Polypropylene Copolymer, Antistatic An antistated polypropylene random copolymer produced by Ineos utilizing unique catalyst technology. It is designed for blowmolding and extrusion applications and exhibits good stiffness and improv.. |
|||
Tensile Strength, Yield | 26.9 MPa | 3900 psi | ASTM D638 |
Spartech Polypro SP-1710 Co/Pol Polyolefin Sheet Description: Polyolefin SheetInformation provided by Spartech. |
|||
Tensile Strength, Yield | 26.9 MPa | 3900 psi | 2" (50mm) per min; ASTM D638 |
Formosa Plastics Formolene® 6144O Impact Copolymer Polypropylene Impact Copolymer for Appliance Applications Formolene® 6144O is a medium impact copolymer of polypropylene characterized by its easy mold flow, physical property balance and excellent dimensional s.. |
|||
Tensile Strength, Yield | 26.9 MPa | 3900 psi | 2" (50mm) per min.; ASTM D638 Type IV |
Formosa Plastics Formolene® HB5202B2 Sheet and Thermoforming HDPE High Density Polyethylene Hexene CopolymerApplications: Containers for bleach, detergents, chemicals; Molded or formed industrial housings, shrouds and tanks.Formolene HB5202B2 is designed for appli.. |
|||
Tensile Strength, Yield | 26.9 MPa | 3900 psi | ASTM D638 |
Eastman Tenite 307A4000015 Propionate Clear, Trsp Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties if Tenite cellulosi.. |
|||
Tensile Strength, Yield | 26.9 MPa | 3900 psi | ASTM D638 |
Eastman Tenite 360E3V45516 Propionate Water Clear, Trsp Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties of Tenite cellulosi.. |
|||
Tensile Strength, Yield | 26.9 MPa | 3900 psi | ASTM D638 |
Eastman Tenite Propionate 381E4000015 Clear, Trsp Cellulose Acetate Propionate Plasticizer 15%. Weight loss on heating = 0.7% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
Tensile Strength, Yield | 26.9 MPa | 3900 psi | ASTM D638 |
Eastman Tenite Propionate 384A4000016 Clear, Trsp Cellulose Acetate Propionate Plasticizer 16%. Weight loss on heating = 1.3% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
Tensile Strength, Yield | 26.9 MPa | 3900 psi | ASTM D638 |
Chevron Phillips Marlex® 9004 HDPE Injection Molding Resin Resin Type: Linear Copolymer, ASTM D 4976 Classification: PE 233, A 56700Characteristics: Moderate Flow, Excellent Impact Strength, Good Stiffness, Excellent ESCR, Moderate Shrinkage ResistanceAppli.. |
|||
Tensile Strength, Yield | 26.9 MPa | 3900 psi | ASTM D638 |
Chevron Phillips Marlex® 9006 HDPE Injection Molding Resin Resin Type: Linear Copolymer, ASTM D 4976 Classification: PE 233, A 56700Characteristics: Moderate Flow, Excellent Impact Strength, Good Stiffness, Excellent ESCR, Moderate Shrinkage ResistanceAppli.. |
|||
Tensile Strength, Yield | 26.9 MPa | 3900 psi | ASTM D638 |
ExxonMobil Paxon™ AB50-003 Blow Molding Resin Product Description: AB50-003 is a blow molding grade high density polyethylene copolymer. This resin has very good stress crack resistance combined with high impact strength and rigidity.Availabili.. |
|||
Tensile Strength, Yield | 26.9 MPa | 3900 psi | ASTM D638 |
Dow 6D20 Polypropylene Random Copolymer Resin OverviewConsistent processabilityGood regrind stabilityGood gloss and clarityLow odor and taste transferComplies with: U.S. FDA 21 CFR 177.1520 (c)3.1a, Europe EU-Directive 2002/72/ECDOW 6D20 Polypr.. |
|||
Tensile Strength, Yield | 26.9 MPa | 3900 psi | Molded and tested in accordance with ASTM D4976; ASTM D638 |
Dow DMDA-8940 NT 7 High Density Polyethylene Resin DOW DMDA-8940 NT 7 is produced using UNIPOL™ process technology. It is intended for use in a broad range of injection molding applications such as housewares, toys, food containers and pails. Info.. |
|||
Tensile Strength, Yield | 26.9 MPa | 3900 psi | Molded and tested in accordance with ASTM D4976; ASTM D638 |
Dow UNIVAL™ DMDA-6200 NT 7 High Density Polyethylene Resin (HDPE) Moderate swell Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a UNIVAL™ DMDA-6200 NT 7 is a multipurpose polymer designed for high speed production of blow molded containers used to package househol.. |
|||
Tensile Strength, Yield | 26.9 MPa | 3900 psi | ASTM D638 |
ExxonMobil Paxon™ AF50-003 Blow Molding Resin AProduct Description: AF50-003 is a blow molding high density polyethylene copolymer containing an antistatic additive. It offers very good balance of stress crack resistance, stiffness and impact s.. |
|||
Tensile Strength, Yield | 26.9 MPa | 3900 psi | ASTM D638 |
Dow R132-02A Polypropylene Random Copolymer Resin DOW R132-02A Polypropylene Resin is a random copolymer intended for use in extrusion blow molding applications. The product can be used in both single layer and multilayer designs including barrier.. |
|||
Tensile Strength, Yield | 26.9 MPa | 3900 psi | 2 in/min (50 mm/min); ASTM D-638 |
Bapolene® PP5026 Polypropylene, Extrusion/Injection Grade Polypropylene extrusion impact copolymer with excellent color and processability. This resin also has a superior balance of stiffness and impact strength. This product meets FDA regulation 21 CFR .. |
|||
Tensile Strength, Yield | 26.9 MPa | 3900 psi | 2 in/min (50 mm/min); ASTM D638 |
Bapolene® PP5052 Polypropylene, Injection Grade Polypropylene injection impact copolymer with excellent color and processability. This resin also has a superior balance of stiffness and impact strength. This product meets FDA standards for food.. |
|||
Tensile Strength, Yield | 26.9 MPa | 3900 psi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 10 PHR N774 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Tensile Strength, Yield | 26.9 MPa | 3900 psi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 10 PHR N774 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |