Material Notes:
Grade H05H-01 is a homopolymer polypropylene for injection molding applications. It is an excellent long-term heat aging grade and offers superior extraction resistance in hot aqueous solutions. This makes it an excellent candidate for use in washing machines, dishwashers, and cofffee makers. This material has been recognized by UL for sustained use at 130c and meets the requirements of the Food and Drug Administration as specified in 21 CFR 177.1520 and is Drug Master file listed.Suggested fabrication methods: Injection moldingFeatures: Heat resistance, Long-term heat agingTypical applications: Appliances, CompoundingComplies with FDA specification, Title 21, CFR 177.1520.Typical property data below from injection molded samples.
Physical Properties Metric English Comments
Density 0.886 - 0.926 g/cc
0.0320 - 0.0335 lb/in³
ASTM D1505
Water Absorption <= 0.010 %
<= 0.010 %
24 hours; ASTM D570
Linear Mold Shrinkage 0.010 - 0.025 cm/cm
0.010 - 0.025 in/in
ASTM D955
Melt Flow 5.7 g/10 min

@Load 2.16 kg,
Temperature 230 °C
5.7 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 79 - 108
79 - 108
Normal range for injection molding resins; ASTM D785
Tensile Strength, Yield 36.0 MPa
5220 psi
ASTM D638
Elongation at Break 200 %
200 %
ASTM D638
Elongation at Yield 9.0 %
9.0 %
ASTM D638
Flexural Modulus 1.38 GPa
200 ksi
ASTM D790A
Izod Impact, Notched 0.200 - 0.300 J/cm

@Diameter 3.17 mm
0.375 - 0.562 ft-lb/in

@Diameter 0.125 in
bar; ASTM D256
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 130 °C
266 °F
UL Relative Thermal Index
Deflection Temperature at 0.46 MPa (66 psi) 93.0 °C
199 °F
ASTM D648
Flammability, UL94 HB
HB
Descriptive Properties Value Comments
Process Injection Molding
Region Mexico
Bamberger Polymers Distribution
US & Canada
Bamberger Polymers Distribution
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved