Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.923 - 0.926 g/cc | 0.0333 - 0.0335 lb/in³ | ASTM D1505 |
Petroquimica Triunfo Trithene® TN 7006 LDPE - Coextruded Film The Trithene® TS 7006 resin is a low-density polyethylene (LDPE) with high molecular weight and very good clarity. The unique combination of good processability, bubble stability, gloss, and streng.. |
|||
Density | 0.923 - 0.926 g/cc | 0.0333 - 0.0335 lb/in³ | ASTM D1505 |
Petroquimica Triunfo Trithene® TS 7006 LDPE - Coextruded Film The Trithene TS 7006 resin is a low-density polyethylene (LDPE) with high molecular weight and very good clarity. The unique combination of good processability, bubble stability, gloss, and strength.. |
|||
Density | 0.920 - 0.926 g/cc | 0.0332 - 0.0335 lb/in³ | ASTM D1505 |
Petroquimica Triunfo Trithene® TS 8064 LDPE - Packaging Film The Trithene TS 8064 resin is a low-density polyethylene (LDPE) with a medium molecular weight an excellent processability. Furthermore, this product has good mechanical properties, average transpar.. |
|||
Density | 0.886 - 0.926 g/cc | 0.0320 - 0.0335 lb/in³ | Average value: 0.903 g/cc Grade Count:89 |
Overview of materials for Polypropylene, Fiber Grade This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Fiber Grade". Each property range of values reported is minimum and maximum values of app.. |
|||
Density | 0.886 - 0.926 g/cc | 0.0320 - 0.0335 lb/in³ | ASTM D1505 |
Ineos H13G-00 Polypropylene Homopolymer
(discontinued **) Formerly Amoco® 7444. Suggested fabrication methods: Injection moldingFeatures: General purposeTypical applications: Rigid packaging, Medical componentsComplies with FDA specification, Title 21, C.. |
|||
Density | 0.886 - 0.926 g/cc | 0.0320 - 0.0335 lb/in³ | ASTM D1505 |
Ineos H00M-01 Polypropylene Homopolymer
(discontinued **) Suggested fabrication methods: Extrusion; ThermoformingFeatures: High melt strength, High stiffness, Medium-term heat agingComplies with FDA specification, Title 21, CFR 177.1520.Typical application.. |
|||
Density | 0.886 - 0.926 g/cc | 0.0320 - 0.0335 lb/in³ | ASTM D1505 |
Ineos H00M-00 Polypropylene Homopolymer
(discontinued **) Suggested fabrication methods: Extrusion; ThermoformingFeatures: High melt strength, Enhanced flow, Medium-term heat agingComplies with FDA specification, Title 21, CFR 177.1520.Typical applications.. |
|||
Density | 0.886 - 0.926 g/cc | 0.0320 - 0.0335 lb/in³ | ASTM D1505 |
Ineos H20Z-01 Polypropylene Homopolymer
(discontinued **) Suggested fabrication methods: Injection moldingFeatures: Nucleated, AntistaticTypical applications: Rigid packaging, Consumer productsComplies with FDA specification, Title 21, CFR 177.1520.Typical.. |
|||
Density | 0.886 - 0.926 g/cc | 0.0320 - 0.0335 lb/in³ | ASTM D1505 |
BP Amoco Amoco® 7942 Polypropylene Homopolymer
(discontinued **) Suggested fabrication methods: Injection moldingFeatures: Excellent mold release, AntistaticTypical applications: Closures, Thin-walled rigid packagingComplies with FDA specification, Title 21, CFR .. |
|||
Density | 0.886 - 0.926 g/cc | 0.0320 - 0.0335 lb/in³ | ASTM D1505 |
Ineos H38G-01 Polypropylene Homopolymer, Fiber Grade
(discontinued **) Suggested fabrication methods: Fiber spinningFeatures: Very high speed spinning, Low gas fadeTypical applications: Spunbound fabricsComplies with FDA specification, Title 21, CFR 177.1520.Typical pr.. |
|||
Density | 0.886 - 0.926 g/cc | 0.0320 - 0.0335 lb/in³ | ASTM D1505 |
BP Amoco Acctuf® 3045 Impact Copolymer Polypropylene
(discontinued **) Suggested fabrication methods: Extrusion; Compression; Injection moldingFeatures: Medium-term heat aging; UL recognizedComplies with FDA specification, Title 21, CFR 177.1520.Typical property data .. |
|||
Density | 0.886 - 0.926 g/cc | 0.0320 - 0.0335 lb/in³ | ASTM D1505 |
BP Amoco Acctuf® 3119HS Ultra High Impact Copolymer Polypropylene
(discontinued **) Suggested fabrication methods: Extrusion; ThermoformingFeatures: High stiffness, Low Temperature impactComplies with FDA specification, Title 21, CFR 177.1520.Typical property data below from inject.. |
|||
Density | 0.886 - 0.926 g/cc | 0.0320 - 0.0335 lb/in³ | ASTM D1505 |
BP Amoco Acctuf® 3143 Impact Copolymer Polypropylene
(discontinued **) Suggested fabrication methods: Sheet extrusion; Thick-wall Injection moldingFeatures: General purposeComplies with FDA specification, Title 21, CFR 177.1520.Typical property data below from injectio.. |
|||
Density | 0.886 - 0.926 g/cc | 0.0320 - 0.0335 lb/in³ | ASTM D1505 |
Ineos H03G-00 Polypropylene Homopolymer Suggested fabrication methods: ExtrusionFeatures: Low water carry-overTypical applications: Woven fabric, Cordage, Slit filmComplies with FDA specification, Title 21, CFR 177.1520.Typical property d.. |
|||
Density | 0.886 - 0.926 g/cc | 0.0320 - 0.0335 lb/in³ | ASTM D1505 |
Ineos H13M-00 Polypropylene Homopolymer Grade H13M-00 is a general purpose polypropylene homopolymer for injection molding applications. It provides good long-term heat stability.Suggested fabrication methods: Injection moldingFeatures: .. |
|||
Density | 0.886 - 0.926 g/cc | 0.0320 - 0.0335 lb/in³ | ASTM D1505 |
Ineos H20H-00 Polypropylene Homopolymer This resin is designed to provide easy moldability for applications requiring resistance to long term heating. This material has been recognized by UL for sustained use at 130c.Suggested fabricatio.. |
|||
Density | 0.890 - 0.926 g/cc | 0.0322 - 0.0335 lb/in³ | Average value: 0.921 g/cc Grade Count:22 |
Overview of materials for Linear Low Density Polyethylene (LLDPE), Compounding Resin This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE), Compounding Resin". Each property range of values reported is m.. |
|||
Density | 0.886 - 0.926 g/cc | 0.0320 - 0.0335 lb/in³ | ASTM D1505 |
Ineos H05H-01 Polypropylene Homopolymer Grade H05H-01 is a homopolymer polypropylene for injection molding applications. It is an excellent long-term heat aging grade and offers superior extraction resistance in hot aqueous solutions. T.. |
|||
Density | 0.886 - 0.926 g/cc | 0.0320 - 0.0335 lb/in³ | ASTM D1505 |
BP Amoco Accpro® 9346 Enhanced Polypropylene
(discontinued **) Suggested fabrication methods: Injection moldingFeatures: Long-term heat aging, High stiffness, Nucleated, UL RecognizedComplies with FDA specification, Title 21, CFR 177.1520.Typical applications: .. |
|||
Density | 0.886 - 0.926 g/cc | 0.0320 - 0.0335 lb/in³ | ASTM D1505 |
BP Amoco Accpro® 9433 Enhanced Polypropylene
(discontinued **) Suggested fabrication methods: Injection moldingFeatures: High stiffness, Surface hardness, Stain resistance, Antistatic, NucleatedComplies with FDA specification, Title 21, CFR 177.1520.Typical app.. |
|||
Density | 0.886 - 0.926 g/cc | 0.0320 - 0.0335 lb/in³ | ASTM D1505 |
BP Amoco Accpro® 9961 Enhanced Polypropylene
(discontinued **) Suggested fabrication methods: Injection moldingFeatures: NucleatedTypical applications: CompoundingComplies with FDA specification, Title 21, CFR 177.1520.Typical property data below from injection.. |
|||
Density | 0.886 - 0.926 g/cc | 0.0320 - 0.0335 lb/in³ | ASTM D1505 |
BP Amoco Acctuf® 3541 Impact Copolymer Polypropylene
(discontinued **) Suggested fabrication methods: Injection moldingFeatures: General purpose, High melt flowComplies with FDA specification, Title 21, CFR 177.1520.Typical property data below from injection molded sam.. |
|||
Density | 0.886 - 0.926 g/cc | 0.0320 - 0.0335 lb/in³ | ASTM D1505 |
BP Amoco Acclear® 8439 Random Copolymer Polypropylene, High Clarity Grade
(discontinued **) Suggested fabrication methods: Injection molding; Stretch blow moldingFeatures: Ultra high clarity, Good impact, Low bloomingTypical applications: Housewares, Rigid packagingComplies with FDA specif.. |
|||
Density | 0.886 - 0.926 g/cc | 0.0320 - 0.0335 lb/in³ | ASTM D1505 |
BP Amoco Acclear® 8449 Random Copolymer Polypropylene, High Clarity Grade
(discontinued **) Suggested fabrication methods: Injection molding; Stretch blow moldingFeatures: Ultra high clarity, Good impact, Excellent static controlTypical applications: Housewares, Rigid packagingComplies wit.. |
|||
Density | 0.886 - 0.926 g/cc | 0.0320 - 0.0335 lb/in³ | ASTM D1505 |
BP Amoco Acclear® 8939 Random Copolymer Polypropylene, High Clarity Grade
(discontinued **) Suggested fabrication methods: Injection molding; Stretch blow moldingFeatures: Ultra high clarity, Excellent static control, ToughenedTypical applications: Housewares, Rigid packaging, Media packag.. |
|||
Density | 0.886 - 0.926 g/cc | 0.0320 - 0.0335 lb/in³ | ASTM D1505 |
Ineos H13Z-00 Polypropylene Homopolymer
(discontinued **) Suggested fabrication methods: Injection moldingFeatures: Nucleated, AntistaticTypical applications: Packaging, Consumer productsComplies with FDA specification, Title 21, CFR 177.1520.Typical prope.. |
|||
Density | 0.886 - 0.926 g/cc | 0.0320 - 0.0335 lb/in³ | ASTM D1505 |
BP Amoco Amoco® 6361 Polypropylene Homopolymer
(discontinued **) Suggested fabrication methods: Extrusion; Blow moldingFeatures: Ease of processingTypical applications: Oriented film, Sheet, Fiber, Profile, Consumer productsComplies with FDA specification, Title .. |
|||
Density | 0.886 - 0.926 g/cc | 0.0320 - 0.0335 lb/in³ | ASTM D1505 |
BP Amoco Amoco® Polypropylene Homopolymer
(discontinued **) Suggested fabrication methods: Injection molding; Rotary CompressionFeatures: Nucleated, Antistatic, LubricatedTypical applications: Closures, CapsComplies with FDA specification, Title 21, CFR 177... |
|||
Density | 0.886 - 0.926 g/cc | 0.0320 - 0.0335 lb/in³ | ASTM D1505 |
Ineos H38K-00 Polypropylene Homopolymer, Fiber Grade
(discontinued **) Suggested fabrication methods: Fiber spinningFeatures: Very high speed spinning, Low gas fade, Low smokeTypical applications: Spunbound fabricsComplies with FDA specification, Title 21, CFR 177.1520.. |
|||
Density | 0.886 - 0.926 g/cc | 0.0320 - 0.0335 lb/in³ | ASTM D1505 |
BP Amoco Acctuf® 3434 Impact Copolymer Polypropylene
(discontinued **) Suggested fabrication methods: Injection moldingFeatures: High gloss, Nucleated, AntistaticComplies with FDA specification, Title 21, CFR 177.1520.Typical property data below from injection molded s.. |