Ineos B50-35H-011 HDPE

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE
Manufacturer Ineos Olefins & Polymers USA
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ineos B50-35H-011 HDPE.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Ineos B50-35H-011 is a high density polyethylene copolymer developed for blow molding applications. It is recommended for use in applications which require a combination of high top load strength and good environmental stress crack resistance (ESCR). This material meets the Food and Drug Administration requirements of 21CFR 177.1520.
Physical Properties Metric English Comments
Density 0.950 g/cc
0.0343 lb/in³
ASTM D4883
Melt Flow 0.35 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.35 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 65
65
ASTM D2240
Tensile Strength, Yield 25.5 MPa
3700 psi
2 in/min (50 mm/min); ASTM D-638
Elongation at Break 700 %
700 %
2 in/min (50 mm/min); ASTM D-638
Flexural Modulus 0.600 GPa
87.0 ksi
ASTM D747
1.103 GPa
160.0 ksi
Tangent; ASTM D 790
Izod Impact, Notched 1.90 J/cm
3.56 ft-lb/in
ASTM D256
Tensile Impact Strength 302 kJ/m²
144 ft-lb/in²
ASTM D1822
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 70.0 °C
158 °F
ASTM D648
Vicat Softening Point 130 °C
266 °F
ASTM D1525
Brittleness Temperature <= -75.0 °C
<= -103 °F
ASTM D746
Descriptive Properties Value Comments
Process Blow Molding
Users viewing this material also viewed the following: