Indium Corp. Indalloy 149 Tin-Lead Solder Alloy

Category Metal , Nonferrous Metal , Lead Alloy , Solder/Braze Alloy
Manufacturer Indium Corporation of America
Trade Name Indalloy
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Indium Corp. Indalloy 149 Tin-Lead Solder Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information Provided by Indium Corporation
Physical Properties Metric English Comments
Density 10.21 g/cc
0.3689 lb/in³
Mechanical Properties Metric English Comments
Hardness, Brinell 11
11
Tensile Strength at Break 33.1 MPa
4800 psi
Elongation at Break 20 %
20 %
Modulus of Elasticity 20.0 GPa
2900 ksi
Shear Strength 20.7 MPa
3000 psi
Thermal Properties Metric English Comments
CTE, linear 27.0 µm/m-°C

@Temperature 20.0 °C
15.0 µin/in-°F

@Temperature 68.0 °F
Thermal Conductivity 37.0 W/m-K

@Temperature 85.0 °C
257 BTU-in/hr-ft²-°F

@Temperature 185 °F
Melting Point 183 - 280 °C
361 - 536 °F
Solidus 183 °C
361 °F
Liquidus 280 °C
536 °F
Component Elements Properties Metric English Comments
Lead, Pb 80 %
80 %
Tin, Sn 20 %
20 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.0000198 ohm-cm
0.0000198 ohm-cm