Thermal Properties | Metric | English | Comments |
---|---|---|---|
Liquidus | 280 °C | 536 °F | |
Indium Corp. Indalloy 149 Tin-Lead Solder Alloy Information Provided by Indium Corporation |
|||
Liquidus | 280 °C | 536 °F | |
Indium Corp. Indalloy® 182 Au-Sn Solder Alloy Eutectic die attach and package sealing.Information provided by the manufacturer, Indium Corporation. |
|||
Liquidus | 280 °C | 536 °F | Flow Point |
Lucas-Milhaupt Clean & Bright 6 Tin/ Silver Solder Characteristics:This alloy is considered to be high strength solders. It has much higher creep strengths than the tin/lead solders. It is a good color match for stainless steel, and used with the p.. |
|||
Liquidus | 280 °C | 536 °F | |
Williams Advanced Alloys Wambraze™ WB280 80Au/20Sn Solder High-purity vacuum cast materials are manufactured by Williams in a variety of solder alloys, including gold brazing alloys for electronic packaging and high temperature joining vacuum electronic de.. |
|||
Liquidus | 280 °C | 536 °F | |
Williams Advanced Alloys WS280A Solder All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys |
|||
Liquidus | 280 °C | 536 °F | |
Williams Advanced Alloys WS280B Solder (Au80/Sn20) All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys |
|||
Liquidus | 280 °C | 536 °F | |
AIM 80Au/20Sn Solder for Photonic Packaging Uses include:Fiber to Ferrule SolderingLaser Die AttachHermetic Packaging & SealingWetting & Sealing Laser OpticsThermal ManagementInformation provided by AIM Specialty Materials. |