Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 0.0000198 ohm-cm | 0.0000198 ohm-cm | |
Indium Corp. Indalloy 149 Tin-Lead Solder Alloy Information Provided by Indium Corporation |
|||
Electrical Resistivity | 0.0000198 ohm-cm | 0.0000198 ohm-cm | Annealed |
Eagle Brass 706 Copper Nickel 10%, 1/2 Hard 706 exhibits excellent corrosion resistance, especially in marine applications. It has a relatively high strength and has resistance at elevated temperatures. The cost is relatively high compared to.. |
|||
Electrical Resistivity | 0.0000198 ohm-cm | 0.0000198 ohm-cm | Annealed |
Eagle Brass 706 Copper Nickel 10%, 1/4 Hard 706 exhibits excellent corrosion resistance, especially in marine applications. It has a relatively high strength and has resistance at elevated temperatures. The cost is relatively high compared to.. |
|||
Electrical Resistivity | 0.0000198 ohm-cm | 0.0000198 ohm-cm | Annealed |
Eagle Brass 706 Copper Nickel 10%, Annealed 706 exhibits excellent corrosion resistance, especially in marine applications. It has a relatively high strength and has resistance at elevated temperatures. The cost is relatively high compared to.. |
|||
Electrical Resistivity | 0.0000198 ohm-cm | 0.0000198 ohm-cm | Annealed |
Eagle Brass 706 Copper Nickel 10%, Extra Hard 706 exhibits excellent corrosion resistance, especially in marine applications. It has a relatively high strength and has resistance at elevated temperatures. The cost is relatively high compared to.. |
|||
Electrical Resistivity | 0.0000198 ohm-cm | 0.0000198 ohm-cm | Annealed |
Eagle Brass 706 Copper Nickel 10%, Hard 706 exhibits excellent corrosion resistance, especially in marine applications. It has a relatively high strength and has resistance at elevated temperatures. The cost is relatively high compared to.. |
|||
Electrical Resistivity | 0.0000198 ohm-cm | 0.0000198 ohm-cm | Annealed |
Eagle Brass 706 Copper Nickel 10%, Spring 706 exhibits excellent corrosion resistance, especially in marine applications. It has a relatively high strength and has resistance at elevated temperatures. The cost is relatively high compared to.. |
|||
Electrical Resistivity | 0.0000198 ohm-cm | 0.0000198 ohm-cm | Annealed |
Eagle Brass 762 Nickel Silver 12%, 1/2 Hard 762 is a nickel silver alloy that has excellent strength, stress relaxation resistance, and solderability. Due to it being extremely resistant to corrosion it doesn't tarnish easily and has a long s.. |
|||
Electrical Resistivity | 0.0000198 ohm-cm | 0.0000198 ohm-cm | Annealed |
Eagle Brass 762 Nickel Silver 12%, 1/4 Hard 762 is a nickel silver alloy that has excellent strength, stress relaxation resistance, and solderability. Due to it being extremely resistant to corrosion it doesn't tarnish easily and has a long s.. |
|||
Electrical Resistivity | 0.0000198 ohm-cm | 0.0000198 ohm-cm | Annealed |
Eagle Brass 762 Nickel Silver 12%, 3/4 Hard 762 is a nickel silver alloy that has excellent strength, stress relaxation resistance, and solderability. Due to it being extremely resistant to corrosion it doesn't tarnish easily and has a long s.. |
|||
Electrical Resistivity | 0.0000198 ohm-cm | 0.0000198 ohm-cm | Annealed |
Eagle Brass 762 Nickel Silver 12%, Annealed 762 is a nickel silver alloy that has excellent strength, stress relaxation resistance, and solderability. Due to it being extremely resistant to corrosion it doesn't tarnish easily and has a long s.. |
|||
Electrical Resistivity | 0.0000198 ohm-cm | 0.0000198 ohm-cm | Annealed |
Eagle Brass 762 Nickel Silver 12%, Extra Hard 762 is a nickel silver alloy that has excellent strength, stress relaxation resistance, and solderability. Due to it being extremely resistant to corrosion it doesn't tarnish easily and has a long s.. |
|||
Electrical Resistivity | 0.0000198 ohm-cm | 0.0000198 ohm-cm | Annealed |
Eagle Brass 762 Nickel Silver 12%, Extra Spring 762 is a nickel silver alloy that has excellent strength, stress relaxation resistance, and solderability. Due to it being extremely resistant to corrosion it doesn't tarnish easily and has a long s.. |
|||
Electrical Resistivity | 0.0000198 ohm-cm | 0.0000198 ohm-cm | Annealed |
Eagle Brass 762 Nickel Silver 12%, Hard 762 is a nickel silver alloy that has excellent strength, stress relaxation resistance, and solderability. Due to it being extremely resistant to corrosion it doesn't tarnish easily and has a long s.. |
|||
Electrical Resistivity | 0.0000198 ohm-cm | 0.0000198 ohm-cm | Annealed |
Eagle Brass 762 Nickel Silver 12%, Spring 762 is a nickel silver alloy that has excellent strength, stress relaxation resistance, and solderability. Due to it being extremely resistant to corrosion it doesn't tarnish easily and has a long s.. |