Material Notes:
Good pre-tinning alloyInformation Provided by Indium Corporation
Physical Properties Metric English Comments
Density 8.16 g/cc
0.295 lb/in³
Mechanical Properties Metric English Comments
Hardness, Brinell 17
17
Tensile Strength at Break 53.8 MPa
7800 psi
Elongation at Break 30 %
30 %
Modulus of Elasticity 35.0 GPa
5080 ksi
Shear Strength 35.9 MPa
5200 psi
Thermal Properties Metric English Comments
CTE, linear 22.0 µm/m-°C

@Temperature 20.0 °C
12.2 µin/in-°F

@Temperature 68.0 °F
Melting Point 183 - 186 °C
361 - 367 °F
Solidus 183 °C
361 °F
Liquidus 186 °C
367 °F
Component Elements Properties Metric English Comments
Lead, Pb 30 %
30 %
Tin, Sn 70 %
70 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.0000138 ohm-cm
0.0000138 ohm-cm