Mechanical Properties Metric English Comments
Tensile Strength at Break 53.8 MPa
7800 psi
2 in/min; ASTM D638
RheTech Products F37-01 40% Glass Fiber/Mineral Co-Reinforced Polypropylene, Chemically Coupled, Black
Applications: ElectronicsBracketsBattery traysInjection molding conditions reported in table.Information provided by RheTech Products.
Tensile Strength at Break 53.8 MPa
7800 psi
2 in/min; ASTM D638
RheTech Products F38-01 35% Glass Fiber/Mineral Co-Reinforced Polypropylene, Chemically Coupled, Black
Applications: Electrical housingsBracketsBattery traysInjection molding conditions reported in table.Information provided by RheTech Products.
Tensile Strength at Break 53.8 MPa
7800 psi
2 in/min; ASTM D638
RheTech Products G13P100-01 13% Glass Fiber Reinforced Polypropylene, Black
Applications: Interior trimAir ducts - distributionFuel filler pocketInjection molding conditions reported in table.Information provided by RheTech Products.
Tensile Strength at Break 53.8 MPa
7800 psi
2 in/min; ASTM D638
RheTech Products G13P100-01UV 13% Glass Fiber Reinforced Polypropylene, UV Stabilized, Black
Applications: Interior trimAir ducts - distributionFuel filler pocketInjection molding conditions reported in table.Information provided by RheTech Products.
Tensile Strength at Break 53.8 MPa
7800 psi
Type I, 5.1 mm/min; ASTM D638
PolyOne Nymax™ GB 1200 30 HS BLACK 18 Polyamide 66 (Nylon 66)
Preliminary Data SheetMolded Test Bars: Dry as MoldedInformation provided by PolyOne
Tensile Strength at Break 53.8 MPa
7800 psi
ASTM D638
Oxford Polymers C-Acetal 10MF-900 BK Acetal
Product Description: Acetal Injection Molding Grade, 10 melt flow Processing and Delivery Form: Pellets and Injection MoldingSpecial Characteristics: Pre-colored blackInformation provided by Oxford..
Tensile Strength at Break 53.8 MPa
7800 psi
ASTM D638
Polymer Resources PC-FR-IM1 Polycarbonate, Preliminary Data Sheet, Low Temperature Impact and Flame Retardant
Process: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Tensile Strength at Break 53.8 MPa
7800 psi
ASTM D638
Polymer Resources PC-IM2 Polycarbonate, Impact Modified, Medium Flow
Polycarbonate, Impact Modified, Medium FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided ..
Tensile Strength at Break 53.8 MPa
7800 psi
ASTM D638
Polymer Resources PC-IM2-UV Polycarbonate, Impact Modified, Medium Flow, UV-stabilized
Polycarbonate, Impact Modified, Medium Flow, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inform..
Tensile Strength at Break 53.8 MPa
7800 psi
Type I, 5.1 mm/min; ASTM D638
PolyOne Edgetek® X TR2-30TA/000 NATURAL Copolyester
The Edgetek™ engineering thermoplastics compounds made with Eastman Tritan™ copolyester offer a wide range of performance and properties with the addition of reinforcing additives. By utilizing Ea..
Tensile Strength at Break 53.8 MPa
7800 psi
2 in/min; ASTM D638
RheTech Products F32-01 32% Glass Fiber/Mineral Co-Reinforced Polypropylene, Chemically Coupled, Black
Applications: Head lamp housingBracketsUnderhood componentsElectrical housingsFunctional supportsInjection molding conditions reported in table.Information provided by RheTech Products.
Tensile Strength at Break 53.8 MPa
7800 psi
ASTM D638
Polymer Resources PC/ABS-GP1-[color]-3 PC Blend, General Purpose, UV-stabilized
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Tensile Strength at Break 53.8 MPa
7800 psi
ASTM D638
Ravago Manufacturing Americas Hylon® N1000STHLUV2 HF Nylon 6/6  (discontinued **)
Available in North America Additive: Heat Stabilizer, Lubricant and UV StabilizerFeatures: Good Toughness, Lubricated, Heat Stabilized and High FlowRoHS CompliantAuto Specifications: GM GMP.PA66.074..
Tensile Strength at Break 53.8 MPa
7800 psi
Indium Corp. Indalloy 108 Tin-Lead Solder Alloy
Good pre-tinning alloyInformation Provided by Indium Corporation
Tensile Strength at Break 53.8 MPa

@Thickness 3.20 mm
7800 psi

@Thickness 0.126 in
Injection Molded; ASTM D638
Styron PULSEâ„¢ 2100 LG PC/ABS Engineering Resin
Overview: PULSE 2100LG Engineering Resin is designed to provide top performance in tough applications, from single piece items to intricate components. Ideal for energy management solutions, it can ..
Tensile Strength at Break 53.8 MPa
7800 psi
ASTM D638
Plastics Group Polifil® GFPP-40 40% Glass-Reinforced Polypropylene
Polifil® GFPP series compounds are homopolymer polypropylene resins reinforced with glass fibers. They provide high impact with increased strength, stiffness, surface hardness, and higher continuou..
Tensile Strength at Break 53.8 MPa
7800 psi
ASTM D638
Chase Plastics CP Pryme® N310GL (COND, 50% RH) Nylon 6 (Utility Grade), 10% Glass Fiber Reinforced, Internally Lubricated
Information provided by Chase Plastics.
Tensile Strength at Break 53.8 MPa
7800 psi
ASTM D638
Plastics Group Polifil® GFPPCC-10 10% Glass Reinforced Polypropylene
Polifil® GFPPCC series compounds are homopolymer polypropylenes reinforced with chemically coupled glass fibers. These compounds offer superior strength and stiffness, improved elevated temperature..
Tensile Strength at Break 53.8 MPa

@Temperature 22.8 °C
7800 psi

@Temperature 73.0 °F
ASTM D638
Ensinger TECAFLON™ PVDF Polyvinylidene Fluoride (PVDF) - extruded products
Polyvinylidene fluoride, or PVDF, is a fluorinated thermoplastic resin which has good resistance to most mineral and organic acids, aliphatic and aromatic hydrocarbons, alcohols, halogenated solvent..
Tensile Strength at Break 53.8 MPa
7800 psi
ASTM D638
Chase Plastics CP Pryme® PCA100 Polycarbonate/ABS Alloy
Information provided by Chase Plastics.