Material Notes:
TRANSIT - A premium molding compound with excellent resistance to flame and smoke generation, high impact strength, and weatherability.Data provided by the manufacturer.
Physical Properties Metric English Comments
Density 1.70 g/cc
0.0614 lb/in³
Water Absorption 0.15 %
0.15 %
in 24 hours; ASTM D570
Linear Mold Shrinkage 0.0010 cm/cm
0.0010 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Barcol 49 - 55
49 - 55
ASTM D2583
Tensile Strength, Ultimate 131 MPa
19000 psi
ASTM D638
Flexural Strength 207 MPa
30000 psi
ASTM D790
Flexural Modulus 13.0 GPa
1890 ksi
ASTM D790
Compressive Strength 234 MPa
33900 psi
ASTM D695
Izod Impact, Notched 15.9 J/cm
29.8 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) >= 260 °C
>= 500 °F
ASTM D648
Flammability, UL94 V-0

@Thickness 3.20 mm
V-0

@Thickness 0.126 in
Electrical Properties Metric English Comments
Dielectric Strength 8.70 kV/mm
221 kV/in
ASTM D149
Arc Resistance 185 sec
185 sec
ASTM D495