Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 131 MPa | 19000 psi | 5.1 mm/min; ASTM D638 |
PolyOne Edgetek® ES-30GF/000 Black Polyethersulfone (PESU) Edgetek™ ES-30GF/000 Black XP120031Information provided by PolyOne |
|||
Tensile Strength, Ultimate | 131 - 200 MPa | 19000 - 29000 psi | Average value: 170 MPa Grade Count:5 |
Overview of materials for Polyetherketoneetherketoneketone (PEKEKK), Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyetherketoneetherketoneketone (PEKEKK), Glass Fiber Filled". Each property range of values reported i.. |
|||
Tensile Strength, Ultimate | 131 MPa | 19000 psi | ASTM D638 |
Technetics Group Amicon™ PEEK 30% Carbon
(Unverified Data**) Information provided by Technetics Group (formerly Plastomer Technologies) |
|||
Tensile Strength, Ultimate | 131 MPa | 19000 psi | ASTM D638 |
PolyOne Edgetek® ES-20GF-15GM/000 Polyethersulfone - 20% Glass Fiber - 15% Milled Glass
(discontinued **) Data provided by PolyOne. |
|||
Tensile Strength, Ultimate | 131 MPa | 19000 psi | |
Premix Premi-Glas® 1200-50VE 1200-50 VE SMC
(discontinued **) Description: Premi-Glas® 1200-50 VE is a sheet molding compound.Market: StructuralInformation provided by Premix. |
|||
Tensile Strength, Ultimate | 131 MPa | 19000 psi | ASTM D638 |
Techmer ES Electrafil® J-3/CF/10 Nylon 6, 10% Carbon Fiber Reinforced |
|||
Tensile Strength, Ultimate | 131 MPa | 19000 psi | ASTM D638 |
Techmer ES Electrafil® J-50/CF/20 Polycarbonate, 20% Carbon Fiber Reinforced Carbon Fiber Reinforced |
|||
Tensile Strength, Ultimate | 131 MPa | 19000 psi | ATSM D638 |
Ashley Polymers Ashlene® 527-33G Nylon 66, 33% Glass Reinforced A 33% glass reinforced impact modified Nylon 66.Data provided by the manufacturer |
|||
Tensile Strength, Ultimate | 131 MPa | 19000 psi | ATSM D638 |
Ashley Polymers Ashlene® 630-33GU Nylon 6, 33% Glass Reinforced Nylon 6, 33% glass reinforced resin, utility grade. Also available: 630S - 33GU Heat Stabilized, 630 - 33GBU Black, 630S - 33GBU Black with H.S.Data provided by the manufacturer |
|||
Tensile Strength, Ultimate | 131 MPa | 19000 psi | ATSM D638 |
Ashley Polymers Ashlene® 68MG Nylon 66, Glass/Mineral reinforced A glass/mineral reinforced nylon offering excellent dimensional stability and rigidity.Data provided by the manufacturer |
|||
Tensile Strength, Ultimate | 131 MPa | 19000 psi | ATSM D638 |
Ashley Polymers Ashlene® 990L-30G Nylon 610, 30% Glass Reinforced 30% glass reinforced for excellent dimensional stability and low water absorption.Data provided by the manufacturer |
|||
Tensile Strength, Ultimate | 131 MPa | 19000 psi | ASTM D638 |
Chem Polymer Durlex 740-10 GB PBT, 40% Short Glass Fiber, 10% Glass Bead Reinforced A 40% short glass fiber, 10% glass bead reinforced PBT, offering a combination of tensile strength, warpage control and dimensional stability for close tolerance applications.Data provided by the ma.. |
|||
Tensile Strength, Ultimate | 131 MPa | 19000 psi | ASTM D638 |
A. Schulman ComAlloy Hiloy® 514 Polycarbonate, Glass Reinforced, UL Data provided by the manufacturer, ComAlloy International Company.40% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Tensile Strength, Ultimate | 131 MPa | 19000 psi | ATSM D638 |
Ashley Polymers Ashlene® 520-33GU Nylon 66, 33% Glass Reinforced Nylon 66, 33% glass reinforced resin, utility grade for non-critical applications. Also available: 520S - 33GU Heat Stabilized, 520 - 33GBU Black, 520S - 33GBU Black with H.S.Data provided by the m.. |
|||
Tensile Strength, Ultimate | 131 MPa | 19000 psi | ASTM D638 |
PolyOne Lubri-Tech™ NI-30GF/15T Nylon 6/10 - 30% Glass Fiber Reinforced - 15% PTFE Lubricated
(discontinued * Data provided by PolyOne. |
|||
Tensile Strength, Ultimate | 131 MPa | 19000 psi | ASTM D638 |
PolyOne Stat-Tech™ RA-06CF-09GF/000 Polyarylsulfone - 9% Glass Fiber - 6% Carbon Fiber Reinforced - ESD Applications
&a Data provided by PolyOne. |
|||
Tensile Strength, Ultimate | 131 MPa | 19000 psi | ASTM D638 |
Custom Resins Vexel™ E20GF30 FR , 30% Glass Reinforced, Flame Retardant PET
(discontinued **) Description: Vexel™ E20GF30 FR is a 30% glass fiber reinforced, flame retardant PET. Information provided by Custom Resins. |