Material Notes:
Features:Good processing characteristicsExcellent toughness and environmental stress crackingHigh glossApplicationsThermoformed containers and lids for food packagingCustom extruded sheetABS replacementInformation provided by I. Stern & Co. Inc.
Physical Properties Metric English Comments
Melt Flow 3.5 g/10 min
3.5 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 24.1 MPa
3500 psi
ASTM D638
Elongation at Yield 55 %
55 %
ASTM D638
Flexural Strength 43.4 MPa
6300 psi
ASTM D790
Flexural Modulus 2.14 GPa
310 ksi
ASTM D790
Izod Impact, Notched 1.71 J/cm
3.20 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Vicat Softening Point 97.8 °C
208 °F
ASTM D1525
Flammability, UL94 HB

@Thickness 1.50 mm
HB

@Thickness 0.0591 in
HB

@Thickness 3.00 mm
HB

@Thickness 0.118 in
Optical Properties Metric English Comments
Gloss 90 %
90 %
ASTM D523