Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 97.8 °C | 208 °F | ASTM D1525 |
Global D-2024 Low Density Polyethylene, Film Extrusion Grade
(discontinued **) Description-transparency, high toughness, flexibility, high impact strength, good chemical resistanceApplications-bagsMeets FDA requirements as listed in food additives regulation 21 CFR 117.1520 fo.. |
|||
Vicat Softening Point | 97.8 °C | 208 °F | ASTM D1525 |
I. Stern SH432HG High Impact Polystyrene Extrusion Grade Features:Good processing characteristicsExcellent toughness and environmental stress crackingHigh glossApplicationsThermoformed containers and lids for food packagingCustom extruded sheetABS replace.. |
|||
Vicat Softening Point | 97.8 °C | 208 °F | 50°C/h 50N |
Ineos ABS Lustran® PG 298 Key Features:UnfilledPlatableSuitable processing methods:Injection molding |
|||
Vicat Softening Point | 97.8 °C @Load 1.02 kg |
208 °F @Load 2.25 lb |
120°C/h; ASTM D 1525 |
Styrolution PS 5600/5601 HIPS Fine balance of toughness and rigidityGood processabilityUSP Class VI certifiedUL Classification 94 HBInformation provided by Styrolution |
|||
Vicat Softening Point | 97.8 °C | 208 °F | ASTM D 1525 |
Styrolution Clearblend 145 MBS Clearblend 145 is an impact modified styrene acrylic copolymer blend with excellent clarity.Excellent clarityLow densityEase of processingLow moisture absorptionInformation provided by Styrolution |
|||
Vicat Softening Point | 97.8 °C @Load 1.02 kg |
208 °F @Load 2.25 lb |
120°C/h; ASTM D 1525 |
Styrolution PS 2610 GPPS Extruded packaging; Thermoforming applicationsExcellent toughnessHigh melt strengthGood flow and processabilityInformation provided by Styrolution |
|||
Vicat Softening Point | 97.8 °C | 208 °F | ASTM D1525 |
Teknor Apex Sinvicomp DBS 8607A Polyvinyl Chloride, Rigid Availability: Asia Pacific Features: Good Impact Resistance Uses: Piping Forms: Powder Processing Method: ExtrusionInformation Provided by Teknor Apex |
|||
Vicat Softening Point | 97.8 °C | 208 °F | ASTM D1525 |
Teknor Apex Sinvicomp SRP 9613 Polyvinyl Chloride, Rigid Availability: Asia Pacific Features: Good Impact Resistance Uses: Profiles Forms: Granules Processing Method: ExtrusionInformation Provided by Teknor Apex |
|||
Vicat Softening Point | 97.8 °C | 208 °F | ASTM D1525 |
Total PSC 529 Polystyrene Polystyrene 529 is a medium flow crystal specially formulated for mar resistance. The easy to process crystal minimizes visual defects from ejection and automated part handling. Typical applications.. |
|||
Vicat Softening Point | 97.8 °C | 208 °F | ASTM D1525 |
Total PSI 935E Polystyrene Polystyrene 935E is a high impact polystyrene exhibiting exceptional toughness for sheet and thermoforming applications.This polymer is an excellent choice for cups, food packaging, custom sheet and.. |
|||
Vicat Softening Point | 97.8 °C | 208 °F | ASTM D1525 |
American Polymers API 410 Polystyrene API 410 is a low impact polystyrene with very high gloss and superior dimensional stability.Applications: API 410 is ideally suited for point of purchase displays where high gloss and some impact i.. |
|||
Vicat Softening Point | 97.8 °C | 208 °F | Rate A (50°C/h), Loading 1 (10 N); ASTM D1525 |
Entec Hypel® PELD50/.924 LDPE Available in North America Features: Food Contact Acceptable and Low DensityAgency Ratings: FDA 21 CFR 176.170, Table 2, Cond. B; Cond. C; Cond. D; Cond. E; Cond. F; Cond. G; Cond. H; and FDA 21 CF.. |
|||
Vicat Softening Point | 97.8 °C | 208 °F | annealed; ASTM D-1525A |
Axiall Suprel® SVA 9812 Rigid PVC, Extrusion Georgia Gulf Suprel® SVA 9812 Alloy is an extrusion grade thermoplastic designed for sheet or profile applications requiring high impact resistance. Key features of Suprel 9812 alloy are flame ret.. |
|||
Vicat Softening Point | 97.8 °C | 208 °F | ASTM D1525 |
Americas Styrenics MC3650 High Heat Crystal Polystyrene Product CharacteristicsImproved cycle times in hard to fill partsExcellent clarity with slight blue tintFood Contact CompliantUL Classification 94HBUSP Class VITypical ApplicationsHousewaresConsumer.. |
|||
Vicat Softening Point | 97.8 °C | 208 °F | ASTM D1525 |
Americas Styrenics STYRON® 693 High Heat Crystal Polystyrene Product CharacteristicsHigh heat resistanceHigh tensile strengthHigh stiffnessFood Contact CompliantUL Classification 94 HBTypical ApplicationsPackaging/Foam disposablesConsumer electronicsInformati.. |
|||
Vicat Softening Point | 97.8 °C | 208 °F | 50°C/hr; 10N; ASTM D1525 |
Arkema Group Solarkote® A200 Acrylic Superior UV protection and weatherability, ASTM Classification PMMA 0233V1Information provided by Arkema Group |
|||
Vicat Softening Point | 97.8 °C | 208 °F | ASTM D1525 |
Teknor Apex Sinvicomp DBS 8615 Polyvinyl Chloride, Rigid Availability: Asia Pacific Features: Good Impact Resistance Uses: Piping Forms: Powder Processing Method: ExtrusionInformation Provided by Teknor Apex |
|||
Vicat Softening Point | 97.8 °C | 208 °F | ASTM D1525 |
Total PSI 975E Polystyrene Polystyrene 975E is a high impact polystyrene designed for extrusion/thermoforming applications. The food ESCR properties of 975E dictate its use for dairy applications that are subjected to high bu.. |
|||
Vicat Softening Point | 97.8 °C | 208 °F | ASTM D1525 |
American Polymers API 392 Polystyrene API 392 is a general purpose polystyrene produced in pellet form for injection molding. API 392 has excellent clarity and high flow.Applications: Used in the manufacture of containers, housewares, .. |