Material Notes:
Chemraz® 592, a versatile perfluoroelastomer developed with a proprietary filler system, is very resistant to plasma attack. This compound’s durometer allows for some hardware finish inconsistency and higher sealing loads. It’s well suited for critical seals in static and dynamic dry applications where reliability and purity are equally essential. Chemraz 592 is recommended for applications with service temperatures up to 240°C (464°F).Applications:Slit valvesLid sealsEndpoint windowsValve sealsWindow sealsIsolator valve sealsGas inlet sealsBell jar sealsKF fitting sealsInformation provided by Greene Tweed.
Physical Properties Metric English Comments
Specific Gravity 2.07 g/cc
2.07 g/cc
ASTM D297
Mechanical Properties Metric English Comments
Hardness, Shore A 80
80
ASTM D2240
Tensile Strength at Break 14.5 MPa
2100 psi
ASTM D1414
Tensile Strength, Yield 4.83 MPa
700 psi
@50% Elongation; ASTM D1414
12.2 MPa
1770 psi
@100% Elongation; ASTM D1414
Elongation at Break 120 %
120 %
ASTM D1414
Compression Set 36 %
36 %
70 hours @ 400°F (204°C) @ 25% deflection; ASTM D395
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 240 °C
464 °F
Minimum Service Temperature, Air -30.0 °C
-22.0 °F
Descriptive Properties Value Comments
Color White