Honeywell Aegis™ PL220HS High Viscosity, Heat Stabilized, Flexible Nylon 6  (discontinued **)

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Heat Stabilized
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Honeywell Aegis™ PL220HS High Viscosity, Heat Stabilized, Flexible Nylon 6  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Aegis PL220HS is a high viscosity, heat stabilized, flexible nylon 6 especially suited to the production of large diameter extrusion or blow molding profiles offering a combination of good flexibility, toughness and abrasion resistance. Chemical resistance is excellent to greases, oils and hydrocarbons.Applications:Used in extruded profile applications.Information provided by Honeywell.
Physical Properties Metric English Comments
Specific Gravity 1.13 g/cc
1.13 g/cc
ASTM D792
Maximum Moisture Content 0.0010
0.0010
Mechanical Properties Metric English Comments
Tensile Strength, Yield 51.0 MPa
7400 psi
ASTM D638
Elongation at Break >= 100 %
>= 100 %
ASTM D638
Flexural Strength 34.0 MPa
4930 psi
ASTM D790
Flexural Modulus 1.00 GPa
145 ksi
ASTM D790
Izod Impact, Notched 1.21 J/cm
2.27 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 220 °C
428 °F
ASTM D3418
Deflection Temperature at 1.8 MPa (264 psi) 53.0 °C
127 °F
ASTM D648
Processing Properties Metric English Comments
Rear Barrel Temperature 230 - 250 °C
446 - 482 °F
Middle Barrel Temperature 240 - 255 °C
464 - 491 °F
Front Barrel Temperature 230 - 250 °C
446 - 482 °F
Die Temperature 230 - 245 °C
446 - 473 °F
Melt Temperature 250 - 260 °C
482 - 500 °F
Head Temperature 230 - 245 °C
446 - 473 °F