Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 1.21 J/cm | 2.27 ft-lb/in | ASTM D256 |
Honeywell Aegis™ PL220HS High Viscosity, Heat Stabilized, Flexible Nylon 6
(discontinued **) Description: Aegis PL220HS is a high viscosity, heat stabilized, flexible nylon 6 especially suited to the production of large diameter extrusion or blow molding profiles offering a combination of g.. |
|||
Izod Impact, Notched | 1.21 J/cm | 2.27 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP RFP38 PA6.6 LNP* LUBRICOMP* RFP38 is a compound based on Nylon 66 containing 40% Glass Fiber, 15% PTFE/Silicone. Added feature of this grade is: Wear Resistant. |