Mechanical Properties Metric English Comments
Izod Impact, Notched 1.21 J/cm
2.27 ft-lb/in
ASTM D256
Honeywell Aegis™ PL220HS High Viscosity, Heat Stabilized, Flexible Nylon 6  (discontinued **)
Description: Aegis PL220HS is a high viscosity, heat stabilized, flexible nylon 6 especially suited to the production of large diameter extrusion or blow molding profiles offering a combination of g..
Izod Impact, Notched 1.21 J/cm
2.27 ft-lb/in
ASTM D256
SABIC Innovative Plastics LNP LUBRICOMP RFP38 PA6.6
LNP* LUBRICOMP* RFP38 is a compound based on Nylon 66 containing 40% Glass Fiber, 15% PTFE/Silicone. Added feature of this grade is: Wear Resistant.