Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | 145 - 150 °C | 293 - 302 °F | Average value: 148 °C Grade Count:4 |
Overview of materials for Polycarbonate, Carbon Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Carbon Fiber Reinforced". Each property range of values reported is minimum and maximum v.. |
|||
Glass Transition Temp, Tg | 145 °C | 293 °F | Tg |
Industrial Laminates/Norplex NP180 Synthetic Fabric
(discontinued **) Description: aramid fabric material with a high performance epoxy resin matrix. Excellent electrical and mechanical properties at elevated temperatures and in adverse environments.Thickness Tested: .. |
|||
Glass Transition Temp, Tg | 145 °C | 293 °F | DMA, ASTM D4065 |
Quantum Composites QC-8100 60% Glass Fiber Vinyl Ester SMC
(discontinued **) QC-8100 is a vinyl ester based sheet molding compound (SMC) designed for compression molding of components requiring high structural strength and corrosion resistance. Form and Colors = Rolled Shee.. |
|||
Glass Transition Temp, Tg | 145 °C | 293 °F | ISO 11357-2 |
Menzolit Menzolit® SMC 1000 Unsaturated Polyester UP SMC 1000 is a special SMC for hydrolysis resistant applications. The glass level has been selected to combine good mouldability with good strength and stiffness properties. Typical applications are .. |
|||
Glass Transition Temp, Tg | 145 °C | 293 °F | TMA |
Lord Adhesives Thermosetâ„¢ ME-541 Underfill Encapsulant LORD Thermosetâ„¢ ME-541 encapsulant is an anhydride free, high purity, semi-conductor grade epoxy underfill product developed for the encapsulation of densely populated area array flip chip devi.. |
|||
Glass Transition Temp, Tg | 145 - 155 °C | 293 - 311 °F | DMA |
Hexcel® HexPly® 1458 160°C-180°C Curing Epoxy Matrix HexPly® 1458 is a self-extinguishing and self-adhesive modified epoxy resin system for monolithic and sandwich structures. HexPly® 1458 has excellent temperature and moisture resistance. It has a .. |
|||
Glass Transition Temp, Tg | 145 °C | 293 °F | |
Covestro Makrolon® 2205 Polycarbonate, Injection Grade Exceptionally good flow injection molding grade with easy mold release, for parts with a low wall thickness and long flow paths.Information provided by Bayer.As of 1 September 2015, Bayer MaterialSc.. |
|||
Glass Transition Temp, Tg | 145 °C | 293 °F | 10°C/min; ISO 11357-1,-2 |
Covestro Makrolon® 2256 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Food contact quality•.. |
|||
Glass Transition Temp, Tg | 145 °C | 293 °F | 10°C/min; ISO 11357-1,-2 |
Covestro Makrolon® 2258 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Medical devices - bioc.. |
|||
Glass Transition Temp, Tg | 145 °C | 293 °F | ISO 11357-1/-2 |
Covestro Makrolon® 2556 Polycarbonate MVR (300 °C/1.2 kg) 14 cm3/10 minEasy releaseGood hydrolysis resistanceInjection moldingAvailable in transparentTranslucent and opaque colorsFood contact gradePreprocessingMax. Water content |
|||
Glass Transition Temp, Tg | 145 °C | 293 °F | ISO 11357-1/-2 |
Covestro Makrolon® 2656 Polycarbonate ISO 7391-PC,MR,(,,)-18-9Global gradeMVR (300 °C/1.2 kg) 12.5 cm3/10 minFood contact qualityMedium viscosityEasy releaseGood hydrolysis resistanceInjection molding - Melt temperature 280 - 320 °CAv.. |
|||
Glass Transition Temp, Tg | 145 °C | 293 °F | ISO 11357-1/-2 |
Covestro Makrolon® 2665 Polycarbonate, Flame Retardant Grade ISO 7391-PC,MFR,(,,)-18-9Global gradeMVR (300 °C/1.2 kg) 12.5 cm3/10 minChlorine- and bromine-free flame retardantUL 94V-2/1.5 mm and 3.0 mmMedium viscosityEasy releaseInjection molding - Melt temp.. |
|||
Glass Transition Temp, Tg | 145 °C | 293 °F | ISO 11357-1/-2 |
Covestro Makrolon® 2856 Polycarbonate ISO 7391-PC,MR,(,,)-09-9Global gradeMVR (300 °C/1.2 kg) 9.5 cm3/10 minFood contact qualityMedium viscosityEasy releaseGood hydrolysis resistanceInjection molding - Melt temperature 280 - 320 °CAva.. |
|||
Glass Transition Temp, Tg | 145 °C | 293 °F | ISO 11357-1/-2 |
Covestro Makrolon® 6455 Polycarbonate, Flame Retardant Grade MVR (300 °C/1.2 kg) 12.5 cm3/10 minUL 94V-0/3.0 mmeasy releaseinjection moldingavailable in transparenttranslucent and opaque colorsPreprocessingMax. Water content |
|||
Glass Transition Temp, Tg | 145 °C | 293 °F | 10°C/min; ISO 11357-1,-2 |
Covestro Makrolon® FU4007 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Furniture applications.. |
|||
Glass Transition Temp, Tg | 145 °C | 293 °F | ISO 11357-1/-2 |
Covestro Makrolon® LQ3187 Polycarbonate ISO 7391-PC,MLR,(,,)-09-9Global gradeMVR (300 °C/1.2 kg) 6.0 cm3/10 minOptical lensHigh viscosityUV stabilizedUV 400 cut offEasy releaseInjection molding - Melt temperature 280 - 320 °CAvailable i.. |
|||
Glass Transition Temp, Tg | 145 - 150 °C | 293 - 302 °F | |
A. Schulman ComAlloy Comtuf® 410 Polycarbonate/Polyester Alloy Data provided by the manufacturer, ComAlloy International Company. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has been integrated into the A Sc.. |
|||
Glass Transition Temp, Tg | 145 - 150 °C | 293 - 302 °F | |
A. Schulman ComAlloy Comtuf® 520 Polycarbonate/Styrenic Alloy Data provided by the manufacturer, ComAlloy International Company. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has been integrated into the A Sc.. |
|||
Glass Transition Temp, Tg | 145 - 150 °C | 293 - 302 °F | |
A. Schulman ComAlloy Comtuf® 523 Polycarbonate/Styrenic Alloy Data provided by the manufacturer, ComAlloy International Company. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has been integrated into the A Sc.. |
|||
Glass Transition Temp, Tg | 145 - 150 °C | 293 - 302 °F | |
A. Schulman ComAlloy Comtuf® 525 Polycarbonate/Styrenic Alloy Data provided by the manufacturer, ComAlloy International Company. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has been integrated into the A Sc.. |
|||
Glass Transition Temp, Tg | 145 - 150 °C | 293 - 302 °F | |
A. Schulman ComAlloy E-16831B Polycarbonate, Electrically Conductive - Carbon Fiber Filled Data provided by the manufacturer, ComAlloy International Company.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Glass Transition Temp, Tg | 145 - 150 °C | 293 - 302 °F | |
A. Schulman ComAlloy Hiloy® 512 Polycarbonate, Glass Reinforced, UL Data provided by the manufacturer, ComAlloy International Company.20% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Glass Transition Temp, Tg | 145 - 150 °C | 293 - 302 °F | |
A. Schulman ComAlloy Hiloy® 515 Polycarbonate, Carbon Fiber Reinforced Data provided by the manufacturer, ComAlloy International Company.10% Carbon Fiber Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Glass Transition Temp, Tg | 145 - 150 °C | 293 - 302 °F | |
A. Schulman ComAlloy Hiloy® 516 Polycarbonate, Carbon Fiber Reinforced Data provided by the manufacturer, ComAlloy International Company.20% Carbon Fiber Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Glass Transition Temp, Tg | 145 - 150 °C | 293 - 302 °F | |
A. Schulman ComAlloy Lubrilon® 511 Polycarbonate, Glass Fiber/PTFE, UL Data provided by the manufacturer, ComAlloy International Company. High performance and excellent lubricity with minimal surface wear.The ComAlloy product line has been integrated into the A Schulma.. |
|||
Glass Transition Temp, Tg | 145 - 150 °C | 293 - 302 °F | |
A. Schulman ComAlloy Comtuf® 524 Polycarbonate/Styrenic Alloy Data provided by the manufacturer, ComAlloy International Company. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has been integrated into the A Sc.. |
|||
Glass Transition Temp, Tg | 145 - 150 °C | 293 - 302 °F | |
A. Schulman ComAlloy Hiloy® 518 Polycarbonate, Carbon Fiber Reinforced Data provided by the manufacturer, ComAlloy International Company.40% Carbon Fiber Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Glass Transition Temp, Tg | 145 °C | 293 °F | ISO 11357-1/-2 |
Covestro Makrolon® LED2245 Polycarbonate ISO 7391-PC,MRT,(,,)-24-9Global gradeFormerly Makrolon DP1-1857MVR (300 °C/1.2 kg) 36 cm3/10 minLight guidesPC with highest transmissionLow viscosityEasy releaseInjection molding - Melt temperature.. |
|||
Glass Transition Temp, Tg | 145 °C | 293 °F | DSC |
Gharda Chemicals GATONE™ 5300PF Polyetheretherketone (PEEK)
(discontinued **) Characteristics: Outstanding Chemical Resistance Outstanding Wear Resistance Outstanding Resistance to HydrolysisExcellent Mechanical Properties Outstanding Thermal properties Very good Dielectric.. |
|||
Glass Transition Temp, Tg | 145 °C | 293 °F | Plain Cast Resin; ASTM D3418 |
TSE Industries EcoWIND® P200G High Performance Filament Winding Polyurethane Resin for Pipes TSE-EcoWIND® resins are “Environmentally-Preferred Products” or EPP’s. They are a pair of polyurethane resins free of Styrene, and are “ultra-low” emitting during application. TSE-EcoWIND® re.. |