Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 3.78 GPa | 548 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Cycolac® INP562 ABS SABIC INP562 provides compatibility with a wider range of ABS grades than many color concentrate bases; allows better dispersion than pellets; allows concentrate manufacturers to produce both pellet.. |
|||
Flexural Modulus | 3.78 GPa | 548 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Cycolac® INP562 ABS+SAN SABIC INP562 provides compatibility with a wider range of ABS grades than many color concentrate bases; allows better dispersion than pellets; allows concentrate manufacturers to produce both pellet.. |
|||
Flexural Modulus | 3.78 GPa | 548 ksi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP MX92284 PP (Asia Pacific) LNP* Thermocomp* MX92284 is a compound based on Polypropylene resin containing Proprietary Filler(s). |
|||
Flexural Modulus | 3.78 GPa | 548 ksi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP RB008 PA 66 (Asia Pacific) LNP THERMOCOMP* RB008 is a compound based on Nylon 66 resin containing Glass Bead. |
|||
Flexural Modulus | 3.78 GPa | 548 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP 2F004 FP-E (EFTE) LNP* FP-EF-1004 is a fluoropolymer compound based on ETFE resin containing 20% Glass Fiber. |
|||
Flexural Modulus | 3.78 GPa | 548 ksi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP MX92284 PP LNP* THERMOCOMP* MX92284 is a compound based on Polypropylene resin containing Proprietary Filler(s). |
|||
Flexural Modulus | 3.78 GPa | 548 ksi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP RB008 PA 66 LNP THERMOCOMP* RB008 is a compound based on Nylon 66 resin containing 40% Glass Bead. |
|||
Flexural Modulus | 3.78 GPa | 548 ksi | ASTM D790 |
Westlake Plastics Imidex Thermoplastic Polyimide Made from Aurum® resin. Applications include electronics, acoustics, composites, wire/cable insulation, adhesive film, and washers/gaskets. It will not melt unto itself, is thermoformable, has hi.. |
|||
Flexural Modulus | 3.78 GPa | 548 ksi | ISO 178 |
Hexcel® HexPly® 916 120°C Curing Epoxy Matrix HexPly® 916 is a self-extinguishing modified epoxy matrix system with very high self adhesive properties. It is an ideal system for single shot honeycomb sandwich manufacture, with good drape chara.. |
|||
Flexural Modulus | 3.78 GPa | 548 ksi | 5% Cloisite® reinforced Nylon 6 |
BYK Cloisite® 10A Nanoclay Cloisite® 10A is an additive for plastics to improve various plastic physical properties, such as reinforcement, HDT, CLTE and barrier.
Information provided by Southern Clay ProductsSouthern Clay P.. |
|||
Flexural Modulus | 3.78 GPa | 548 ksi | 5% Cloisite® reinforced Nylon 6 |
BYK Cloisite® 15A Nanoclay Cloisite® 15A is an additive for plastics to improve various plastic physical properties, such as reinforcement, HDT, CLTE and barrier.Information provided by Southern Clay ProductsSouthern Clay Pr.. |
|||
Flexural Modulus | 3.78 GPa | 548 ksi | 5% Cloisite® reinforced Nylon 6 |
BYK Cloisite® 20A Nanoclay Cloisite® 20A is an additive for plastics to improve various plastic physical properties, such as reinforcement, HDT, CLTE and barrier.Information provided by Southern Clay ProductsSouthern Clay Pr.. |
|||
Flexural Modulus | 3.78 GPa | 548 ksi | 5% Cloisite® reinforced Nylon 6 |
BYK Cloisite® 25A Nanoclay Cloisite® 25A is an additive for plastics to improve various plastic physical properties, such as reinforcement, HDT, CLTE and barrier.Information provided by Southern Clay ProductsSouthern Clay Pr.. |
|||
Flexural Modulus | 3.78 GPa | 548 ksi | 5% Cloisite® reinforced Nylon 6 |
BYK Cloisite® 93A Nanoclay Cloisite® 93A is an additive for plastics to improve various plastic physical properties, such as reinforcement, HDT, CLTE and barrier.Information provided by Southern Clay ProductsSouthern Clay Pr.. |
|||
Flexural Modulus | 3.78 GPa | 548 ksi | 5% Cloisite® reinforced Nylon 6 |
BYK Cloisite® 30B Nanoclay Cloisite® 30B is an additive for plastics to improve various plastic physical properties, such as reinforcement, HDT, CLTE and barrier.
Information provided by Southern Clay ProductsSouthern Clay P.. |
|||
Flexural Modulus | 3.78 GPa | 548 ksi | 5% Cloisite® reinforced Nylon 6 |
BYK Cloisite® Na+ Nanoclay Cloisite® Na+ is an additive for plastics to improve various plastic physical properties, such as reinforcement, HDT, CLTE and barrier.Information provided by Southern Clay ProductsSouthern Clay Pr.. |