Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Henkel Hysol EA 9394 Paste Adhesive System

Category Polymer , Adhesive , Thermoset , Epoxy , Epoxy Adhesive
Manufacturer Henkel
Trade Name Hysol
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Henkel Hysol EA 9394 Paste Adhesive System.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Thixotropic adhesive with structural properties to 350°F / 177°C.Applications: Potting Structural Repair Composite Bonding Liquid Shim
Physical Properties Metric English Comments
Storage Temperature 25.0 °C
77.0 °F
Mechanical Properties Metric English Comments
Tensile Strength 46.0 MPa
6670 psi
Elongation at Break 1.7 %
1.7 %
Tensile Modulus 4.25 GPa
616 ksi
Compressive Strength 158.6 MPa
23000 psi
Adhesive Bond Strength 20.0 MPa

@Temperature 93.0 °C
2900 psi

@Temperature 199 °F
Tensile Lap Shear
22.8 MPa

@Temperature -55.0 °C
3310 psi

@Temperature -67.0 °F
Tensile Lap Shear
29.0 MPa

@Temperature 25.0 °C
4210 psi

@Temperature 77.0 °F
Tensile Lap Shear
Peel Strength 3.60 kN/m
20.5 pli
Bell Peel
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 177 °C
351 °F
Processing Properties Metric English Comments
Cure Time 60.0 min

@Temperature 66.0 °C
1.00 hour

@Temperature 151 °F
7200 - 10100 min

@Temperature 25.0 °C
120 - 168 hour

@Temperature 77.0 °F
Pot Life 100 min
100 min
Descriptive Properties Value Comments
Consistency Thixotropic
Form 2 parts
Mix Ratio, Part A:Part B 100:17
Peel Strength Low
Users viewing this material also viewed the following: