Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Adhesive Bond Strength | 20.0 MPa @Temperature 25.0 °C |
2900 psi @Temperature 77.0 °F |
Lap Shear |
Henkel Hysol EA 9681 Film Adhesive Epoxy film adhesive for bonding applications. Hysol EA9681 is formulated to provide excellent performance properties for many bonding applications, and has excellent results on composite surfaces th.. |
|||
Adhesive Bond Strength | 20.0 MPa @Temperature 121 °C |
2900 psi @Temperature 250 °F |
Lap Shear |
Henkel Hysol PL 777-1FR Film Adhesive Flame retardant, nonmetallic modified epoxy film adhesiveApplications: Metal and Honeycomb Bonding |
|||
Adhesive Bond Strength | 20.0 MPa @Thickness 1.50 mm |
2900 psi @Thickness 0.0591 in |
Lap Shear (CRS St 1203); EN 1465 |
Dow BETAMATE™ 5103-2 Epoxy BETAMATE™ 5103-2 is a one component heat curing Epoxy paste adhesive. The material is readily pumped at ambient temperatures. It shows excellent adhesion to automotive steel, including coated ste.. |
|||
Adhesive Bond Strength | 20.0 MPa @Temperature 23.9 °C |
2900 psi @Temperature 75.0 °F |
on aluminum; ASTM D1002-64 |
3M Pronto™ CA-100 Instant Adhesive One-part, room-temperature curing adhesive that is ready-to-use without metering or mixing. Bonded parts reach handling strength in 5-10 seconds on many applications.Toughened material that provide.. |
|||
Adhesive Bond Strength | 20.0 MPa @Temperature -55.0 °C |
2900 psi @Temperature -67.0 °F |
Tensile Lap Shear |
Henkel Hysol EA 9394.2 Paste Adhesive System Fast cure adhesive for liquid shim and potting. Handling strength within 6 - 8 hours.Applications: Potting Structural Repair Liquid Shim |
|||
Adhesive Bond Strength | 20.0 MPa @Temperature 93.0 °C |
2900 psi @Temperature 199 °F |
Tensile Lap Shear |
Henkel Hysol EA 9394 Paste Adhesive System Thixotropic adhesive with structural properties to 350°F / 177°C.Applications: Potting Structural Repair Composite Bonding Liquid Shim |