Mechanical Properties Metric English Comments
Tensile Modulus 4.25 GPa
616 ksi
Type I, 5.1 mm/min; ASTM D638
PolyOne Geon™ Vinyl Rigid Extrusion L6607 Polyvinyl Chloride, Rigid (PVC, Rigid)
Physical properties based on Geon L6607 white 1363Information provided by PolyOne
Tensile Modulus 4.25 GPa
616 ksi
Radici Radilon® S CV300 (dry) Nylon 6
Radilon® S is a range of polyamide 6 (PA6) products obtained through the polymerization of caprolactam and used for injection, extrusion and blow-molding.Information provided by Radici group.
Tensile Modulus 4.25 GPa
616 ksi
Radici Radilon® A CP300K (cond.) Nylon 66
Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information prov..
Tensile Modulus 4.25 GPa
616 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP THERMOCOMP DF002 PC
LNP THERMOCOMP* DF002 is a compound based on Polycarbonate resin containing 10% Glass Fiber.
Tensile Modulus 4.25 GPa
616 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP THERMOCOMP DF002H PC
LNP THERMOCOMP* DF002H is a compound based on Polycarbonate resin containing 10% Glass Fiber. Added feature includes: Healthcare.
Tensile Modulus 4.25 GPa
616 ksi
Secant; ISO 527-2
ExxonMobil Exxtral™ HMT 402 Performance Polyolefin
Product Description: A specialty thermoplastic polyolefin resin with very high stiffness, high heat ageing resistance and detergent resistance designed for electrical applications such as washing ma..
Tensile Modulus 4.25 GPa
616 ksi
ISO 527
Eurotec® Tecolen® CP30 GR20 NL PPCP, 20% glass fiber reinforced, natural, high flow grade
Information provided by Eurotec®
Tensile Modulus 4.25 GPa
616 ksi
ASTM D638
Azdel SuperLite® SL550800-100 PP Resin Matrix / 55% Glass Fiber (1.5 mm Molded Thickness)
AZDEL SuperLite® SL550800-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic..
Tensile Modulus 4.25 GPa
616 ksi
Henkel Hysol EA 9394 Paste Adhesive System
Thixotropic adhesive with structural properties to 350°F / 177°C.Applications: Potting Structural Repair Composite Bonding Liquid Shim