Material Notes:
H900 is recognized throughout the world as a reliable, consistent GPO-3 material. Standard size sheets are available in thicknesses ranging from .094" to 2.00". H900 also exhibits excellent smoke, flame and toxicity characteristics. Govt. Spec I-24768/6. Standard color - red.Information provided by Haysite
Physical Properties Metric English Comments
Specific Gravity 1.80 g/cc
1.80 g/cc
ASTM D792
Water Absorption 0.20 %
0.20 %
ASTM D229
Mechanical Properties Metric English Comments
Hardness, Barcol 62
62
Tensile Strength 62.1 MPa
9000 psi
ASTM D638
Flexural Strength 124 MPa
18000 psi
ASTM D790
Flexural Modulus 10.3 GPa
1500 ksi
ASTM D790
Compressive Strength 207 MPa
30000 psi
ASTM D695
Shear Strength 96.5 MPa
14000 psi
ASTM D732
Adhesive Bond Strength 9.65 MPa

@Thickness 12.7 mm
1400 psi

@Thickness 0.500 in
ASTM D229
Izod Impact, Notched 4.27 J/cm
8.00 ft-lb/in
Edgewise; ASTM D256
Thermal Properties Metric English Comments
Maximum Service Temperature, Inert 160 °C
320 °F
Flammability, UL94 V-0
V-0
Smoke Density 4.0 min
4.0 min
0.33 Optical Density; ASTM E661
Electrical Properties Metric English Comments
Dielectric Constant 5.2

@Frequency 60.0 Hz
5.2

@Frequency 60.0 Hz
ASTM D150
Dielectric Strength 17.7 kV/mm
450 kV/in
Perpendicular, short time in oil; ASTM D149
Dielectric Breakdown 55000 V
55000 V
Parallel, Step-By-Step in Oil; ASTM D149
Dissipation Factor 0.060

@Frequency 60.0 Hz
0.060

@Frequency 60.0 Hz
ASTM D150
Arc Resistance 190 sec
190 sec
ASTM D495
Comparative Tracking Index >= 600 V
>= 600 V
Descriptive Properties Value Comments
Flame Resistance 130 seconds
Ignition Time, ASTM D229
33 seconds
Burning Time, ASTM D229
Inline Plane Track Resistance 1000 mins
ASTM D2303
Radiant Panel 5
ASTM E162
Tunnel Test <25
1/4", ASTM E84