Thermal Properties Metric English Comments
Smoke Density 4.0 min
4.0 min
<20; ASTM E662
Rogers Corporation Bisco® MF1 6535 - 35 Silicone, High Performance Foam, Indentation Force Material
MF1® 6535 is a high quality silicone foam material designed for a wide range of applications. It features exceptional flame, smoke and toxicity (FST) characteristics, superior weather- and UV-resi..
Smoke Density 4.0 min
4.0 min
<20; ASTM E662
Rogers Corporation Bisco® MF1 8055 - 55 Silicone, High Performance Foam, Indentation Force Material
MF1® 8055 is a high quality silicone foam material designed for a wide range of cushioning and sealing applications. It features exceptional flame, smoke and toxicity (FST) characteristics, superi..
Smoke Density 4.0 min
4.0 min
<20; ASTM E662
Rogers Corporation Bisco® MF1 9575 - 75 Silicone, High Performance Foam, Indentation Force Material
MF1® 9575 is a high quality silicone foam material designed for a wide range of cushioning and sealing applications. It features exceptional flame, smoke and toxicity (FST) characteristics, superi..
Smoke Density 4.0 min
4.0 min
6.3 Optical Density; ASTM E661
Haysite H1000 Polyester Laminate
Haysite Grade 1000 laminate sheet is an outstanding material that is used in applications requiring exceptional weather and corrosion resistance. Grade H1000's unique polyester resin system provide..
Smoke Density 4.0 min
4.0 min
0.33 Optical Density; ASTM E661
Haysite H900 Polyester, Glass Reinforced
H900 is recognized throughout the world as a reliable, consistent GPO-3 material. Standard size sheets are available in thicknesses ranging from .094" to 2.00". H900 also exhibits excellent smoke,..
Smoke Density 4.0 min
4.0 min
<50; ASTM E662
ACC Magnifoam™ MF1-6535™ MTI Silicones Silicone Foam
Part of the Amber Chemical Group. Data provided by manufacturer.
Smoke Density 4.0 min
4.0 min
<50; ASTM E662
ACC Magnifoam™ MF1-8055™ MTI Silicones Silicone Foam
Part of the Amber Chemical Group. Data provided by manufacturer.
Smoke Density 4.0 min
4.0 min
<50; ASTM E662
ACC Magnifoam™ MF1-9575™ MTI Silicones Silicone Foam
Part of the Amber Chemical Group. Data provided by manufacturer.
Smoke Density 4.0 min
4.0 min
<50; ASTM E662
ACC Magnifoam™ MFSILTEC™ Roll Stock MTI Silicones Silicone Foam
Part of the Amber Chemical Group. Data provided by manufacturer.
Smoke Density 4.0 min
4.0 min
<50; ASTM E662
ACC Magnifoam™ MFSILTEC™-HD MTI Silicones Silicone Foam
Part of the Amber Chemical Group. Data provided by manufacturer.
Smoke Density 4.0 min
4.0 min
<50; D<sub>s</sub>; ASTM E662
Rogers Corporation Bisco® BF-2000 Ultra-Soft Silicone Foam
BISCO® Ultra Soft is a highly compressible silicone foam. The combination of low weight and softness makes this flame retardant foam ideal for transportation, industrial and electronics applicatio..