Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Breakdown | 55000 V | 55000 V | |
XP Phenolic Laminate Paper based phenolic provides low cost electrical and mechanical properties. It is widely used for switchboards, panel boards, insulating washers, and intricate punched parts.Information provided b.. |
|||
Dielectric Breakdown | 55000 V @Thickness 1.57 mm |
55000 V @Thickness 0.0620 in |
Cond A; ASTM D229 S/S |
Industrial Laminates/Norplex NP310HT Cotton Fabric Description: Canvas machining grade for structural and mechanical applications. Better impact strength than phenolic paper grades. MIL-I-24768/16. Designed to meet GE specification A19B15B1Thickness.. |
|||
Dielectric Breakdown | 55000 V @Thickness 1.57 mm |
55000 V @Thickness 0.0620 in |
Cond A; ASTM D229 S/S |
Industrial Laminates/Norplex NP615 Paper Base Laminate Description: Room temperature punching and shearing grade up to .125" thick. More flexible and lower mechanical properties than NP611. NP615 is produced with high resin content melamine impregnated .. |
|||
Dielectric Breakdown | 55000 V | 55000 V | Parallel, Step-By-Step in Oil; ASTM D149 |
Haysite H900 Polyester, Glass Reinforced H900 is recognized throughout the world as a reliable, consistent GPO-3 material. Standard size sheets are available in thicknesses ranging from .094" to 2.00". H900 also exhibits excellent smoke,.. |
|||
Dielectric Breakdown | 55000 V | 55000 V | Parallel, Step-By-Step in Oil; ASTM D149 |
Haysite HTF Polyester, High Temp Flex HTF exhibits excellent flexibility and retention of electrical properties at elevated temperatures. For use in 220º C insulation systems in dry type transformers and where flexibility and high te.. |
|||
Dielectric Breakdown | 55000 V @Thickness 1.57 mm |
55000 V @Thickness 0.0620 in |
Cond A; ASTM D229 S/S |
Industrial Laminates/Norplex NP612 Paper Base Laminate Description: Room temperature punching and shearing grade up to .125" thick. More flexible and lower mechanical properties than NP611. Intended for applications where electrical and moisture require.. |
|||
Dielectric Breakdown | >= 55000 V @Temperature 90.0 °C |
>= 55000 V @Temperature 194 °F |
In oil, parallel to laminations; IEC 1212-2 6.2 |
Hippe EP PC 301 Woven Polyester Cloth Reinforced Epoxy Resin - Sheet Used in electrical and mechanical applications. Good resistance to SF6.Information provided by Hippe. |