Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Haysite 14200 Polyester BMC, 15% Glass Reinforced

Category Polymer , Thermoset , Filled/Reinforced Thermoset , Polyester, TS , Thermoset Polyester Glass Filled BMC
Manufacturer Haysite
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Haysite 14200 Polyester BMC, 15% Glass Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
The 14200 series bulk molding compound is one of Haysite's newest molding compound families. This grade can be compression, transfer, or injection molded. Good mechanical strength and exceptional arc/track properties make this grade a natural for many electrical applications. The 14200 BMC is recognized by UL with a 94V-0 flame rating at 0.120" wall thickness (pending).
Physical Properties Metric English Comments
Density 1.85 g/cc
0.0668 lb/in³
ASTM D572
Water Absorption 0.16 %
0.16 %
ASTM D570
Linear Mold Shrinkage 0.0010 cm/cm
0.0010 in/in
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 41.0 MPa
5950 psi
Flexural Strength 138 MPa
20000 psi
Compressive Strength 97.0 MPa
14100 psi
Izod Impact, Notched 4.30 J/cm
8.06 ft-lb/in
edgewise; ASTM D256
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 130 °C
266 °F
temperature rating
Flammability, UL94 V-0
V-0
UL94 V-0 Pending; File No.E-27875
Electrical Properties Metric English Comments
Dielectric Strength 16.0 kV/mm
406 kV/in
Perpendicular (ASTM D149), Short Time
Arc Resistance 194 sec
194 sec
ASTM D495
Comparative Tracking Index 600 V
600 V