Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 97.0 MPa | 14100 psi | ASTM D695 |
Owens Corning Glass Fiber Reinforced Acrylonitrile Butadiene Styrene (ABS), 20 wt.% glass ABS is highly resistant to weak acids and alkalis, and provides good resistance to most organic solvents. It is attacked by sulfuric and nitric acids, and is soluble in esters, ketones and ethylene .. |
|||
Compressive Strength | 97.0 MPa | 14100 psi | ASTM D695 |
Owens Corning Glass Fiber Reinforced Polycarbonate, 10 wt.% glass Data provided by the manufacturer, Owens Corning. |
|||
Compressive Strength | 97.0 MPa | 14100 psi | ASTM D695 |
Glastic Laminates/Shapes FHT Flexible High Temperature Polyester Laminate Data provided by Glastic Corporation.Excellent flexibility plus good electrical strength retention values after long term heat aging. Widely used in motors and dry type transformers. |
|||
Compressive Strength | 97.0 MPa | 14100 psi | |
Haysite 14200 Polyester BMC, 15% Glass Reinforced The 14200 series bulk molding compound is one of Haysite's newest molding compound families. This grade can be compression, transfer, or injection molded. Good mechanical strength and exceptional a.. |
|||
Compressive Strength | 97.0 MPa | 14100 psi | Transverse; ASTM D695 |
Glastic Laminates/Shapes MTS Grade MTS Fiberglass-Reinforced Polyester Rod Data provided by Glastic Corporation.A continuous-filament fiberglass-roving provides superior strength. |
|||
Compressive Strength | 97.0 MPa | 14100 psi | Transverse; ASTM D695 |
Glastic Laminates/Shapes SG-200 Fiberglass-Reinforced Polyester Rod Data provided by Glastic Corporation.A continuous-filament fiberglass-roving provides superior strength. Excellent thermal endurance - used to replace silicone rod. |
|||
Compressive Strength | 97.0 MPa @Strain 3.50 % |
14100 psi @Strain 3.50 % |
DIN EN ISO 604 |
Wolf Kunststoff ZEDEX® ZX-100MT A1T Polymer Alloy, Mineral Reinforced Stiff; Hard; Very high strength; No fiber reinforcementApplications: Handling, Vessel and Pump, Steel and Water, Chemical Engineering, Automotive Technology, Machine ToolsInformation provided by Zed.. |
|||
Compressive Strength | 97.0 MPa | 14100 psi | Absolute Drying; ASTM-D695 |
Toyobo GLAMIDE® TY-145TZ Nylon-6 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |