Haveg 41N Phenolic; Silicate Reinforced Ablative Material

Category Polymer , Thermoset , Filled/Reinforced Thermoset , Phenolic , Phenolic, Ablative Coating
Manufacturer Haveg
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Haveg 41N Phenolic; Silicate Reinforced Ablative Material.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A proprietary thermoset plastic consisting of a phenol-formaldehyde resin and non-asbestos silicate fillers converted to a permanent thermoset state under heat and pressure. It is designed for ablative uses involving heat.
Physical Properties Metric English Comments
Density 1.85 g/cc
0.0668 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 40.4 MPa
5860 psi
Elongation at Break 0.75 %
0.75 %
Tensile Modulus 9.30 GPa
1350 ksi
Flexural Yield Strength 67.8 MPa
9830 psi
Compressive Yield Strength 157 MPa
22800 psi
Thermal Properties Metric English Comments
CTE, linear 9.40 µm/m-°C

@Temperature 20.0 °C
5.22 µin/in-°F

@Temperature 68.0 °F
in x- and y-directions
15.4 µm/m-°C

@Temperature 20.0 °C
8.56 µin/in-°F

@Temperature 68.0 °F
in z-direction
CTE, linear, Transverse to Flow 9.40 µm/m-°C

@Temperature 20.0 °C
5.22 µin/in-°F

@Temperature 68.0 °F
Specific Heat Capacity 1.10 J/g-°C
0.263 BTU/lb-°F
Thermal Conductivity 0.320 W/m-K
2.22 BTU-in/hr-ft²-°F